Materials / Aluminum

Aluminum 5052-H32

Aluminum 5052-H32 strength, stiffness, density and thermal properties, with their source.

A bracket in Aluminum 5052-H32, brushed finish.

ProcessWrought
Mechanical
Yield strength195MPasourcetypical, 0.2% offset
Ultimate tensile strength230MPasourcetypical
Elongation at break12%sourcetypical
Young's modulus (stiffness)70GPasourcetypical
Density2,685kg/m³sourcenominal
Strength to weight72.6kN·m/kg
Stiffness to weight26.1MN·m/kg
Poisson's ratio0.33sourcetypical (handbook physical constant)
Shear modulus26.3GPa
Bulk modulus68.6GPa
Speed of sound5,106m/s
Thermal
Thermal conductivity138W/m·Ksourcebase material: 5052 in O temper (same alloy, annealed); Kaiser typical
Thermal expansion23.8µm/m·Ksourcetypical, mean 20-100 °C
100 mm part over a 50 °C swing119µm growth
Specific heat963J/kg·Ksourceat 100 °C (212 °F); table covers O, H32, H34, H36, H38
Heats up and cools (diffusivity)53.4mm²/s
Thermal shock resistance10,822W/m
Melting point605–650°Csourcemelting range
Values for5052-H32, Kaiser Aluminum tube & pipe typical datasheet (mechanical, CTE, melting); MIL-HDBK-5J (Poisson, density, specific heat)

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 5052-H32
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 5052-H32
Strength against density

Compare Aluminum 5052-H32 with