Brass C260Wrought
SLA Resin Elastic 50A3D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength345MPasourcenominal, strip/flat, 0.5% extension (not 0.2% offset)not given (tensile used)
Ultimate tensile strength427MPasourcenominal, strip/flat3.4MPasourcetypical
Elongation at break23%sourcenominal, in 2.0 in., strip/flat160%sourcetypical
Young's modulus (stiffness)110GPasourcetypical, temper-independentnot sourced
Density8,525kg/m³sourcenominal1,010kg/m³sourcetypical
Strength to weight40.5kN·m/kg12x higher3.37kN·m/kg
Stiffness to weight12.9MN·m/kgnot sourced
Poisson's ratio0.34sourcereference value at room temperature (Wieland-M30 = CuZn30 = C26000, rolled products)not sourced
Shear modulus41.2GPanot sourced
Bulk modulus115GPanot sourced
Speed of sound3,597m/snot sourced
Thermal
Thermal conductivity121W/m·Ksourcetypical, 20 °Cnot sourced
Thermal expansion20µm/m·Ksourcetypical, mean 20-300 °Cnot sourced
100 mm part over a 50 °C swing100µm growthnot sourced
Specific heat377J/kg·Ksourcetypical, 20 °Cnot sourced
Heats up and cools (diffusivity)37.7mm²/snot sourced
Thermal shock resistance12,510W/mnot sourced
Melting point916–954°Csourcesolidus-liquidusnot sourced
Glass transitionnot sourced-34.5°CsourceDMA
Values forC26000 cartridge brass, H02 half hard flat/strip: CDA Electronic Connector Design Guide (mechanical) + CDA alloy page (physical)Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Brass C260 stronger than SLA Resin Elastic 50A?

Brass C260 is stronger: its yield strength is 345 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (101x).

Which is lighter, Brass C260 or SLA Resin Elastic 50A?

SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 8,525 kg/m³ for Brass C260.

Which is lighter for the same job, Brass C260 or SLA Resin Elastic 50A?

For the same stiffness or strength: Brass C260 is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beBrass C260SLA Resin Elastic 50A
Strong rod or tielighter12x heavier
Strong beamlighter2.58x heavier
Strong panel or platelighter19% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrass C260
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickBrass C260SLA Resin Elastic 50A
Strength against density