Materials / Compare

Concrete vs. SLS PA12 Nylon

Compare Concrete vs. SLS PA12 Nylon strength, stiffness, weight and thermal properties.

Change either side
ConcreteCast
SLS PA12 Nylon3D printed (SLS)
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot sourcednot given (tensile used)
Ultimate tensile strengthnot sourced48MPasourcetypical
Compressive strength27.6MPasourcespecified compressive strength class (f'c), not a measured typicalnot sourced
Elongation at breaknot sourced18%sourcetypical
Young's modulus (stiffness)not sourced1.65GPasourcetypical
Density2,240–2,400kg/m³sourcerange for normalweight concrete930kg/m³sourcetypical
Strength to weightnot sourced51.6kN·m/kg
Stiffness to weightnot sourced1.77MN·m/kg
Poisson's ratio0.15–0.2sourcegeneral range at normal ambient conditions (overall 0.11-0.32)not sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourced1,332m/s
Thermal
Thermal conductivity0.9W/m·Ksourcetypical (comparative value)not sourced
Thermal expansion8–12µm/m·Ksourcetypical range for portland cement concrete (aggregate dependent)not sourced
100 mm part over a 50 °C swing50µm growthnot sourced
Specific heat900J/kg·Ksourcetypical (NIST guidance for thermal analysis)not sourced
Heats up and cools (diffusivity)0.431mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Melting pointnot sourced176°Csourcetypical
Max service temperature65°Csourcecode long-term temperature limit (ASME Code, concrete containments)64°CsourceHDT 1.8 MPa, X orientation
Values forNormal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC reviewEOS PA 2200 (PA12) Material Data Sheet, process parameter 'Balance' at 120 µm layer thickness, X orientation, dry (conditioned values not given). Live MDS status 04.10.2026, last changed 10.09.2026; PDF via ?topdf=... link on the same page.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLS PA12 Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Which is lighter, Concrete or SLS PA12 Nylon?

SLS PA12 Nylon is lighter: 930 kg/m³ against 2,320 kg/m³ for Concrete.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000DMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelSLS PA12 Nylon
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ADMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickSLS PA12 Nylon
Strength against density

Related comparisons