Materials / Compare

Concrete vs. Plastic PEEK

Compare Concrete vs. Plastic PEEK strength, stiffness, weight and thermal properties.

Change either side
ConcreteCast
Plastic PEEKBulk polymer (molded or machined)
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot sourced98MPasourcetypical, tensile yield
Ultimate tensile strengthnot sourcednot sourced
Compressive strength27.6MPasourcespecified compressive strength class (f'c), not a measured typical125MPasourcetypical, 23 C
Flexural strengthnot sourced165MPasourcetypical, flexural stress at yield, 23 C
Elongation at breaknot sourced25%sourcetypical, at break
Young's modulus (stiffness)not sourced4GPasourcetypical (nominal)
Density2,240–2,400kg/m³sourcerange for normalweight concrete1,300kg/m³sourcetypical (crystalline)
Strength to weightnot sourced75.4kN·m/kg
Stiffness to weightnot sourced3.08MN·m/kg
Poisson's ratio0.15–0.2sourcegeneral range at normal ambient conditions (overall 0.11-0.32)0.38sourcetypical
Shear modulusnot sourced1.45GPa
Bulk modulusnot sourced5.56GPa
Speed of soundnot sourced1,754m/s
Thermal
Thermal conductivity0.9W/m·Ksourcetypical (comparative value)0.29W/m·Ksourcetypical, average, 23 C
Thermal expansion8–12µm/m·Ksourcetypical range for portland cement concrete (aggregate dependent)55µm/m·Ksourceaverage of flow/cross-flow, below Tg (<143 C)
100 mm part over a 50 °C swing50µm growth5.5x less275µm growth
Specific heat900J/kg·Ksourcetypical (NIST guidance for thermal analysis)2,200J/kg·Ksourcetypical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)
Heats up and cools (diffusivity)0.431mm²/s4.25x faster0.101mm²/s
Thermal shock resistancenot sourced80.1W/m
Melting pointnot sourced343°Csourcetypical, DSC
Glass transitionnot sourced143°Csourceonset (midpoint 150 C)
Max service temperature65°Csourcecode long-term temperature limit (ASME Code, concrete containments)240°CsourceUL 746B RTI, mechanical strength (continuous use index)
Values forNormal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC reviewVictrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Which is lighter, Concrete or Plastic PEEK?

Plastic PEEK is lighter: 1,300 kg/m³ against 2,320 kg/m³ for Concrete.

Which conducts heat better, Concrete or Plastic PEEK?

Concrete conducts heat better: 0.9 W/m·K against 0.29 W/m·K for Plastic PEEK.

Which expands less with temperature?

Concrete expands less: 10 µm/m·K against 55 µm/m·K for Plastic PEEK.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PEEK
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PEEK
Strength against density

Related comparisons