Mechanical
Yield strengthnot sourcednot given (tensile used)
Ultimate tensile strengthnot sourced23.7MPasourcetypical, stress at break
Compressive strength27.6MPasourcespecified compressive strength class (f'c), not a measured typicalnot sourced
Flexural strengthnot sourced4.1MPasourcetypical
Elongation at breaknot sourcednot sourced
Young's modulus (stiffness)not sourced0.067GPasourcetypical
Density2,240–2,400kg/m³sourcerange for normalweight concrete1,220kg/m³sourcetypical
Strength to weightnot sourced19.4kN·m/kg
Stiffness to weightnot sourced0.0549MN·m/kg
Poisson's ratio0.15–0.2sourcegeneral range at normal ambient conditions (overall 0.11-0.32)not sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourced234m/s
Thermal
Thermal conductivity0.9W/m·Ksourcetypical (comparative value)not sourced
Thermal expansion8–12µm/m·Ksourcetypical range for portland cement concrete (aggregate dependent)not sourced
100 mm part over a 50 °C swing50µm growthnot sourced
Specific heat900J/kg·Ksourcetypical (NIST guidance for thermal analysis)not sourced
Heats up and cools (diffusivity)0.431mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Melting pointnot sourced217°Csourcetypical
Max service temperature65°Csourcecode long-term temperature limit (ASME Code, concrete containments)50.3°CsourceHDT 0.455 MPa (printed specimens)
Values forNormal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC reviewUltimaker TPU 95A, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 29, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic TPU is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Which is lighter, Concrete or Plastic TPU?

Plastic TPU is lighter: 1,220 kg/m³ against 2,320 kg/m³ for Concrete.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic TPU
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic TPU
Strength against density

Related comparisons