Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: Cleveland-Cliffs, LyondellBasell, National Institute of Standards and Technology, INEOS Olefins & Polymers USA
Iron
Cleveland-Cliffs / AK Steel ARMCO Pure Iron Product Data Bulletin (07/2022): Table 1 typical physical properties, Table 2 typical mechanical properties after SRA/recrystallization anneal.
Plastic Polypropylene
LyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO values
1
ARMCO Pure Iron Product Data Bulletin (2022)Cleveland-Cliffsarchived copyIron · Yield strength: typical (0.2% YS), hot rolled + SRA/recrystallization annealIron · Ultimate tensile strength: typical, SRA/recrystallization annealIron · Elongation at break: typical, gauge 4D0Iron · Young's modulus (stiffness): typical, after SRA/recrystallization annealIron · Density: typicalIron · Thermal conductivity: typical at 20 °CIron · Thermal expansion: mean, 20-399 °CIron · Specific heat: typicalIron · Melting point: typical
2
Moplen HP501H Product DataLyondellBasellPlastic Polypropylene · Yield strength: typical, tensile stress at yield ISO 527Plastic Polypropylene · Young's modulus (stiffness): typical, tensile modulus ISO 527Plastic Polypropylene · Density: typical, 23 °C ISO 1183-1Plastic Polypropylene · Max service temperature: HDT 0.45 MPa (ISO 75B), unannealed
3
Elastic Properties of Metals and Alloys, I. Iron, Nickel, and Iron-Nickel Alloys, J. Phys. Chem. Ref. Data 2 (1973)National Institute of Standards and Technologyarchived copyIron · Poisson's ratio: NIST critically evaluated best value (polycrystalline iron)
4
Typical Engineering Properties of PolypropyleneINEOS Olefins & Polymers USAarchived copyPlastic Polypropylene · Poisson's ratio: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)Plastic Polypropylene · Thermal conductivity: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)Plastic Polypropylene · Thermal expansion: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Iron stronger than Plastic Polypropylene?
Iron is stronger: its yield strength is 186 MPa against 33 MPa for Plastic Polypropylene (5.64x).
Which is lighter, Iron or Plastic Polypropylene?
Plastic Polypropylene is lighter: 900 kg/m³ against 7,860 kg/m³ for Iron.
Which is stiffer, Iron or Plastic Polypropylene?
Iron is stiffer: Young's modulus 207 GPa against 1.45 GPa for Plastic Polypropylene, so the same part in Iron deflects less under the same load.
Which is lighter for the same job, Iron or Plastic Polypropylene?
For the same stiffness or strength: Iron is lighter for a stiff rod or tie (tension), stiff beam (bending); Plastic Polypropylene is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Iron
Plastic Polypropylene
Stiff rod or tie (tension)
lighter
16.3x heavier
Stiff beam (bending)
lighter
37% heavier
Stiff panel or plate
1.67x heavier
lighter
Strong rod or tie
1.55x heavier
lighter
Strong beam
2.76x heavier
lighter
Strong panel or plate
3.68x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Iron or Plastic Polypropylene?
Iron conducts heat better: 73.2 W/m·K against 0.195 W/m·K for Plastic Polypropylene.
Which expands less with temperature?
Iron expands less: 13.7 µm/m·K against 90 µm/m·K for Plastic Polypropylene.