Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Cleveland-Cliffs, UltiMaker, National Institute of Standards and Technology
Iron
Cleveland-Cliffs / AK Steel ARMCO Pure Iron Product Data Bulletin (07/2022): Table 1 typical physical properties, Table 2 typical mechanical properties after SRA/recrystallization anneal.
Plastic TPU
Ultimaker TPU 95A, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 29, 2022.
1
ARMCO Pure Iron Product Data Bulletin (2022)Cleveland-Cliffsarchived copyIron · Yield strength: typical (0.2% YS), hot rolled + SRA/recrystallization annealIron · Ultimate tensile strength: typical, SRA/recrystallization annealIron · Elongation at break: typical, gauge 4D0Iron · Young's modulus (stiffness): typical, after SRA/recrystallization annealIron · Density: typicalIron · Thermal conductivity: typical at 20 °CIron · Thermal expansion: mean, 20-399 °CIron · Specific heat: typicalIron · Melting point: typical
Elastic Properties of Metals and Alloys, I. Iron, Nickel, and Iron-Nickel Alloys, J. Phys. Chem. Ref. Data 2 (1973)National Institute of Standards and Technologyarchived copyIron · Poisson's ratio: NIST critically evaluated best value (polycrystalline iron)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Plastic TPU is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Iron stronger than Plastic TPU?
Iron is stronger: its yield strength is 186 MPa against tensile strength 23.7 MPa for Plastic TPU (7.85x).
Which is lighter, Iron or Plastic TPU?
Plastic TPU is lighter: 1,220 kg/m³ against 7,860 kg/m³ for Iron.
Which is stiffer, Iron or Plastic TPU?
Iron is stiffer: Young's modulus 207 GPa against 0.067 GPa for Plastic TPU, so the same part in Iron deflects less under the same load.
Which is lighter for the same job, Iron or Plastic TPU?
For the same stiffness or strength: Iron is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie; Plastic TPU is lighter for a strong beam, strong panel or plate.
Part that must be
Iron
Plastic TPU
Stiff rod or tie (tension)
lighter
480x heavier
Stiff beam (bending)
lighter
8.63x heavier
Stiff panel or plate
lighter
2.26x heavier
Strong rod or tie
lighter
22% heavier
Strong beam
1.63x heavier
lighter
Strong panel or plate
2.3x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).