Materials / Compare

SLS PA12 Nylon vs. Wood

Compare SLS PA12 Nylon vs. Wood strength, stiffness, weight and thermal properties.

Change either side
SLS PA12 Nylon3D printed (SLS)
WoodNatural
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength48MPasourcetypical99MPasourcemodulus of rupture (no direct tensile value)
Compressive strengthnot sourced46.6MPasourcecompression parallel to grain (maximum crushing strength), 12% MC
Flexural strengthnot sourced99MPasourcemodulus of rupture (static bending), 12% MC
Elongation at break18%sourcetypicalnot sourced
Young's modulus (stiffness)1.65GPasourcetypical12.5GPasourcebending MOE, parallel to grain
Density930kg/m³sourcetypicalnot sourced
Strength to weight51.6kN·m/kgnot sourced
Stiffness to weight1.77MN·m/kgnot sourced
Poisson's rationot sourced0.35sourcemu_LR (red oak group, ~12% MC)
Shear modulusnot sourced4.63GPa
Bulk modulusnot sourced13.9GPa
Speed of sound1,332m/snot sourced
Thermal
Thermal conductivitynot sourced0.18W/m·Ksourceacross grain, 12% MC (Table 4-7, approximate)
Thermal expansionnot sourced3.1–4.5µm/m·Ksourceparallel to grain, ovendry wood, range across species
100 mm part over a 50 °C swingnot sourced19µm growth
Specific heatnot sourced1,700J/kg·Ksourcesolid wood (all species), 12% MC, 27 C
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistancenot sourced244W/m
Melting point176°Csourcetypicalnot sourced
Max service temperature64°CsourceHDT 1.8 MPa, X orientationnot sourced
Values forEOS PA 2200 (PA12) Material Data Sheet, process parameter 'Balance' at 120 µm layer thickness, X orientation, dry (conditioned values not given). Live MDS status 04.10.2026, last changed 10.09.2026; PDF via ?topdf=... link on the same page.Northern red oak (Quercus rubra), clear straight-grained specimens at 12% MC, parallel to grain unless stated; USDA FPL Wood Handbook FPL-GTR-282 (2021) Ch. 4 and Ch. 5

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLS PA12 Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is SLS PA12 Nylon stronger than Wood?

Wood is stronger: its tensile strength is 99 MPa against 48 MPa for SLS PA12 Nylon (2.06x).

Which is stiffer, SLS PA12 Nylon or Wood?

Wood is stiffer: Young's modulus 12.5 GPa against 1.65 GPa for SLS PA12 Nylon, so the same part in Wood deflects less under the same load.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000DMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelSLS PA12 Nylon
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ADMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickSLS PA12 Nylon
Strength against density