Plastic Polypropylene vs. Plastic TPU

Compare Plastic Polypropylene vs. Plastic TPU strength, stiffness, weight and thermal properties.

Change either side
Plastic PolypropyleneBulk polymer (molded or machined)
Plastic TPU3D printed (FDM)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength33MPasourcetypical, tensile stress at yield ISO 527not given (tensile used)
Ultimate tensile strengthnot sourced23.7MPasourcetypical, stress at break
Flexural strengthnot sourced4.1MPasourcetypical
Elongation at breaknot sourcednot sourced
Young's modulus (stiffness)1.45GPasourcetypical, tensile modulus ISO 5270.067GPasourcetypical
Density900kg/m³sourcetypical, 23 °C ISO 1183-11,220kg/m³sourcetypical
Strength to weight36.7kN·m/kg1.89x higher19.4kN·m/kg
Stiffness to weight1.61MN·m/kg29.3x higher0.0549MN·m/kg
Poisson's ratio0.42sourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)not sourced
Shear modulus0.511GPanot sourced
Bulk modulus3.02GPanot sourced
Speed of sound1,269m/s234m/s
Thermal
Thermal conductivity0.17–0.22W/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)not sourced
Thermal expansion80–100µm/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)not sourced
100 mm part over a 50 °C swing450µm growthnot sourced
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistance28.6W/mnot sourced
Melting pointnot sourced217°Csourcetypical
Max service temperature90°CsourceHDT 0.45 MPa (ISO 75B), unannealed50.3°CsourceHDT 0.455 MPa (printed specimens)
Values forLyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO valuesUltimaker TPU 95A, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 29, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic TPU is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic Polypropylene stronger than Plastic TPU?

Plastic Polypropylene is stronger: its yield strength is 33 MPa against tensile strength 23.7 MPa for Plastic TPU (39%).

Which is lighter, Plastic Polypropylene or Plastic TPU?

Plastic Polypropylene is lighter: 900 kg/m³ against 1,220 kg/m³ for Plastic TPU.

Which is stiffer, Plastic Polypropylene or Plastic TPU?

Plastic Polypropylene is stiffer: Young's modulus 1.45 GPa against 0.067 GPa for Plastic TPU, so the same part in Plastic Polypropylene deflects less under the same load.

Which is lighter for the same job, Plastic Polypropylene or Plastic TPU?

For the same stiffness or strength: Plastic Polypropylene is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PolypropylenePlastic TPU
Stiff rod or tie (tension)lighter29.3x heavier
Stiff beam (bending)lighter6.31x heavier
Stiff panel or platelighter3.78x heavier
Strong rod or tielighter1.89x heavier
Strong beamlighter1.69x heavier
Strong panel or platelighter1.6x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PolypropylenePlastic TPU
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PolypropylenePlastic TPU
Strength against density

Related comparisons