Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: LyondellBasell, Outokumpu, INEOS Olefins & Polymers USA, Steel Construction Institute, Carpenter Technology
Plastic Polypropylene
LyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO values
Stainless Steel 303
1.4305 / UNS S30300, Outokumpu typical values (hot rolled, solution annealed) from 'Steel Grades, Properties and Global Standards'; max service from Carpenter CarTech 303 datasheet
1
Moplen HP501H Product DataLyondellBasellPlastic Polypropylene · Yield strength: typical, tensile stress at yield ISO 527Plastic Polypropylene · Young's modulus (stiffness): typical, tensile modulus ISO 527Plastic Polypropylene · Density: typical, 23 °C ISO 1183-1Plastic Polypropylene · Max service temperature: HDT 0.45 MPa (ISO 75B), unannealed
2
Steel Grades, Properties and Global StandardsOutokumpuarchived copyStainless Steel 303 · Yield strength: Outokumpu typical (product P = hot rolled plate, transverse)Stainless Steel 303 · Ultimate tensile strength: Outokumpu typicalStainless Steel 303 · Elongation at break: Outokumpu typical, A5Stainless Steel 303 · Young's modulus (stiffness): at RT (Table 12)Stainless Steel 303 · Density: at RTStainless Steel 303 · Thermal conductivity: at RTStainless Steel 303 · Thermal expansion: mean, 20–100 °CStainless Steel 303 · Specific heat: at RT
3
Typical Engineering Properties of PolypropyleneINEOS Olefins & Polymers USAarchived copyPlastic Polypropylene · Poisson's ratio: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)Plastic Polypropylene · Thermal conductivity: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)Plastic Polypropylene · Thermal expansion: base material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
4
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 303 · Poisson's ratio: design value (structural stainless steels)
5
Carpenter Stainless Type 303 Data SheetCarpenter Technologyarchived copyStainless Steel 303 · Max service temperature: continuous, scaling limit
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic Polypropylene stronger than Stainless Steel 303?
Stainless Steel 303 is stronger: its yield strength is 275 MPa against 33 MPa for Plastic Polypropylene (8.33x).
Which is lighter, Plastic Polypropylene or Stainless Steel 303?
Plastic Polypropylene is lighter: 900 kg/m³ against 7,900 kg/m³ for Stainless Steel 303.
Which is stiffer, Plastic Polypropylene or Stainless Steel 303?
Stainless Steel 303 is stiffer: Young's modulus 200 GPa against 1.45 GPa for Plastic Polypropylene, so the same part in Stainless Steel 303 deflects less under the same load.
Which is lighter for the same job, Plastic Polypropylene or Stainless Steel 303?
For the same stiffness or strength: Plastic Polypropylene is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 303 is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
Plastic Polypropylene
Stainless Steel 303
Stiff rod or tie (tension)
15.7x heavier
lighter
Stiff beam (bending)
34% heavier
lighter
Stiff panel or plate
lighter
1.7x heavier
Strong rod or tie
lighter
5% heavier
Strong beam
lighter
2.14x heavier
Strong panel or plate
lighter
3.04x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Plastic Polypropylene or Stainless Steel 303?
Stainless Steel 303 conducts heat better: 15 W/m·K against 0.195 W/m·K for Plastic Polypropylene.
Which expands less with temperature?
Stainless Steel 303 expands less: 16 µm/m·K against 90 µm/m·K for Plastic Polypropylene.