Materials / Compare

SLA Resin Elastic 50A vs. Titanium

Compare SLA Resin Elastic 50A vs. Titanium strength, stiffness, weight and thermal properties.

Change either side
SLA Resin Elastic 50A3D printed (SLA resin)
TitaniumWrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)885MPasourcetypical, plate (>0.187 in), annealed, 0.2% offset
Ultimate tensile strength3.4MPasourcetypical940MPasourcetypical, plate, annealed
Elongation at break160%sourcetypical16%sourcetypical, in 2 in., plate annealed
Young's modulus (stiffness)not sourced107–122GPasourcetypical range, 20 °C
Density1,010kg/m³sourcetypical4,430kg/m³sourcenominal
Strength to weight3.37kN·m/kg200kN·m/kg59.3x higher
Stiffness to weightnot sourced25.8MN·m/kg
Poisson's rationot sourced0.342sourcemean of TIMET measurements
Shear modulusnot sourced42.7GPa
Bulk modulusnot sourced121GPa
Speed of soundnot sourced5,084m/s
Thermal
Thermal conductivitynot sourced6.6W/m·Ksourcetypical, 20 °C, mill annealed
Thermal expansionnot sourced9µm/m·Ksourcetypical, mean 0-100 °C
100 mm part over a 50 °C swingnot sourced45µm growth
Specific heatnot sourced580J/kg·Ksourcetypical, 20 °C
Heats up and cools (diffusivity)not sourced2.57mm²/s
Thermal shock resistancenot sourced3,730W/m
Melting pointnot sourced1,630–1,650°Csourcemelting range
Glass transition-34.5°CsourceDMAnot sourced
Max service temperaturenot sourced400°Csourceupper recommended use temperature
Values forFormlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.TIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is SLA Resin Elastic 50A stronger than Titanium?

Titanium is stronger: its yield strength is 885 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (260x).

Which is lighter, SLA Resin Elastic 50A or Titanium?

SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 4,430 kg/m³ for Titanium.

Which is lighter for the same job, SLA Resin Elastic 50A or Titanium?

For the same stiffness or strength: Titanium is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beSLA Resin Elastic 50ATitanium
Strong rod or tie59.3x heavierlighter
Strong beam9.29x heavierlighter
Strong panel or plate3.68x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelTitanium
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickSLA Resin Elastic 50ATitanium
Strength against density

Related comparisons