Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources6 documents: Outokumpu, USDA Forest Products Laboratory, Steel Construction Institute, Carpenter Technology
Stainless Steel 303
1.4305 / UNS S30300, Outokumpu typical values (hot rolled, solution annealed) from 'Steel Grades, Properties and Global Standards'; max service from Carpenter CarTech 303 datasheet
Wood
Northern red oak (Quercus rubra), clear straight-grained specimens at 12% MC, parallel to grain unless stated; USDA FPL Wood Handbook FPL-GTR-282 (2021) Ch. 4 and Ch. 5
1
Steel Grades, Properties and Global StandardsOutokumpuarchived copyStainless Steel 303 · Yield strength: Outokumpu typical (product P = hot rolled plate, transverse)Stainless Steel 303 · Ultimate tensile strength: Outokumpu typicalStainless Steel 303 · Elongation at break: Outokumpu typical, A5Stainless Steel 303 · Young's modulus (stiffness): at RT (Table 12)Stainless Steel 303 · Density: at RTStainless Steel 303 · Thermal conductivity: at RTStainless Steel 303 · Thermal expansion: mean, 20–100 °CStainless Steel 303 · Specific heat: at RT
2
Wood Handbook (FPL-GTR-282), Chapter 5: Mechanical Properties of WoodUSDA Forest Products LaboratoryWood · Ultimate tensile strength: modulus of rupture (no direct tensile value)Wood · Compressive strength: compression parallel to grain (maximum crushing strength), 12% MCWood · Flexural strength: modulus of rupture (static bending), 12% MCWood · Young's modulus (stiffness): bending MOE, parallel to grainWood · Poisson's ratio: mu_LR (red oak group, ~12% MC)
3
Technical Note 218: Weights of Various Woods Grown in the United States (1953)USDA Forest Products LaboratoryWood · Density: average weight of clear wood at 8% and 15% moisture content
4
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 303 · Poisson's ratio: design value (structural stainless steels)
5
Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of WoodUSDA Forest Products LaboratoryWood · Thermal conductivity: across grain, 12% MC (Table 4-7, approximate)Wood · Thermal expansion: parallel to grain, ovendry wood, range across speciesWood · Specific heat: solid wood (all species), 12% MC, 27 C
6
Carpenter Stainless Type 303 Data SheetCarpenter Technologyarchived copyStainless Steel 303 · Max service temperature: continuous, scaling limit
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Stainless Steel 303 stronger than Wood?
Stainless Steel 303 is stronger: its yield strength is 275 MPa against tensile strength 99 MPa for Wood (2.78x).
Which is lighter, Stainless Steel 303 or Wood?
Wood is lighter: 692 kg/m³ against 7,900 kg/m³ for Stainless Steel 303.
Which is stiffer, Stainless Steel 303 or Wood?
Stainless Steel 303 is stiffer: Young's modulus 200 GPa against 12.5 GPa for Wood, so the same part in Stainless Steel 303 deflects less under the same load.
Which is lighter for the same job, Stainless Steel 303 or Wood?
For the same stiffness or strength: Stainless Steel 303 is lighter for a stiff rod or tie (tension); Wood is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Stainless Steel 303
Wood
Stiff rod or tie (tension)
lighter
40% heavier
Stiff beam (bending)
2.86x heavier
lighter
Stiff panel or plate
4.53x heavier
lighter
Strong rod or tie
4.11x heavier
lighter
Strong beam
5.78x heavier
lighter
Strong panel or plate
6.85x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Stainless Steel 303 or Wood?
Stainless Steel 303 conducts heat better: 15 W/m·K against 0.18 W/m·K for Wood.
Which expands less with temperature?
Wood expands less: 3.8 µm/m·K against 16 µm/m·K for Stainless Steel 303.