Silicon

Silicon (single crystal) strength, stiffness, density and thermal properties, with their source.

A panel in Silicon, smooth finish.

ProcessGrown single crystal
Mechanical
Yield strengthnot given (tensile used)
Ultimate tensile strength130MPasourcemodulus of rupture (bending fracture stress); brittle, no yield point
Flexural strength130MPasourcemodulus of rupture
Elongation at breaknot sourced
Young's modulus (stiffness)131GPasourcetypical (single quoted value of an anisotropic crystal)
Density2,329kg/m³sourcetypical
Strength to weight55.8kN·m/kg
Stiffness to weight56.2MN·m/kg
Poisson's ratio0.221sourcetypical
Shear modulus53.6GPa
Bulk modulus78.3GPa
Speed of sound7,500m/s
Thermal
Thermal conductivity163W/m·Ksourcetypical at 313 K (40 °C)
Thermal expansion2.62µm/m·Ksourcetypical at 300 K
100 mm part over a 50 °C swing13.1µm growth
Specific heat732J/kg·Ksourcetypical
Heats up and cools (diffusivity)95.6mm²/s
Thermal shock resistance48,095W/m
Melting point1,412°Csourcetypical
Max service temperature300°Csourceproducer's maximum application temperature (optical components)
Values forSynthetic single-crystal silicon (cubic, diamond structure), Korth Kristalle (crystal grower) material data; Korth usually supplies Floating Zone (FZ) material, Czochralski (Cz) also offered. Silicon is elastically anisotropic; the producer quotes one modulus and the solver is isotropic.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4Ceramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Silicon
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4Ceramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Silicon
Strength against density

Compare Silicon with