Materials / Titanium

Titanium Ti-6Al-4V

Titanium Ti-6Al-4V (Grade 5, annealed) strength, stiffness, density and thermal properties, with their source.

A bracket in Titanium Ti-6Al-4V, brushed finish.

ProcessWrought
Mechanical
Yield strength885MPasourcetypical, plate (>0.187 in), annealed, 0.2% offset
Ultimate tensile strength940MPasourcetypical, plate, annealed
Elongation at break16%sourcetypical, in 2 in., plate annealed
Young's modulus (stiffness)107–122GPasourcetypical range, 20 °C
Density4,430kg/m³sourcenominal
Strength to weight200kN·m/kg
Stiffness to weight25.8MN·m/kg
Poisson's ratio0.342sourcemean of TIMET measurements
Shear modulus42.7GPa
Bulk modulus121GPa
Speed of sound5,084m/s
Thermal
Thermal conductivity6.6W/m·Ksourcetypical, 20 °C, mill annealed
Thermal expansion9µm/m·Ksourcetypical, mean 0-100 °C
100 mm part over a 50 °C swing45µm growth
Specific heat580J/kg·Ksourcetypical, 20 °C
Heats up and cools (diffusivity)2.57mm²/s
Thermal shock resistance3,730W/m
Melting point1,630–1,650°Csourcemelting range
Max service temperature400°Csourceupper recommended use temperature
Values forTIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Brass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Titanium Ti-6Al-4V
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Brass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Titanium Ti-6Al-4V
Strength against density