Materials / Aluminum

Aluminum 1100-O

Aluminum 1100-O (annealed sheet) strength, stiffness, density and thermal properties, with their source.

A panel in Aluminum 1100-O, brushed finish.

ProcessWrought
Mechanical
Yield strength35MPasourcetypical, O, 0.0625 in specimen
Ultimate tensile strength90MPasourcetypical, O
Elongation at break35%sourcetypical, O, in 4D
Young's modulus (stiffness)69GPasourcetypical
Density2,710kg/m³sourcenominal, 20 °C
Strength to weight12.9kN·m/kg
Stiffness to weight25.5MN·m/kg
Poisson's rationot sourced
Shear modulusnot sourced
Bulk modulusnot sourced
Speed of sound5,046m/s
Thermal
Thermal conductivity222W/m·Ksourcetypical, O, 20 °C
Thermal expansion23.6µm/m·Ksourcetypical, mean 20-100 °C
100 mm part over a 50 °C swing118µm growth
Specific heat901J/kg·Ksourcebase material: commercially pure aluminium EN AW-1050A (Hydro), 20 °C
Heats up and cools (diffusivity)90.9mm²/s
Thermal shock resistancenot sourced
Melting point640–655°Csourcemelting range
Values for1100-O (annealed) commercially pure aluminium, Kaiser Aluminum Tube & Pipe Alloy 1100 Technical Data (Rev. 05/06), typical properties; specific heat from Hydro EN AW-1050A (99.5% Al) extruded-products datasheet (10/2018).

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-O
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-O
Strength against density

Compare Aluminum 1100-O with