Materials / Compare

Aluminum 1100-O vs. Concrete

Compare Aluminum 1100-O vs. Concrete strength, stiffness, weight and thermal properties.

Change either side
Aluminum 1100-OWrought
ConcreteCast
Try it on a partA panel to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength35MPasourcetypical, O, 0.0625 in specimennot sourced
Ultimate tensile strength90MPasourcetypical, Onot sourced
Compressive strengthnot sourced27.6MPasourcespecified compressive strength class (f'c), not a measured typical
Elongation at break35%sourcetypical, O, in 4Dnot sourced
Young's modulus (stiffness)69GPasourcetypicalnot sourced
Density2,710kg/m³sourcenominal, 20 °C2,240–2,400kg/m³sourcerange for normalweight concrete
Strength to weight12.9kN·m/kgnot sourced
Stiffness to weight25.5MN·m/kgnot sourced
Poisson's rationot sourced0.15–0.2sourcegeneral range at normal ambient conditions (overall 0.11-0.32)
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound5,046m/snot sourced
Thermal
Thermal conductivity222W/m·Ksourcetypical, O, 20 °C0.9W/m·Ksourcetypical (comparative value)
Thermal expansion23.6µm/m·Ksourcetypical, mean 20-100 °C8–12µm/m·Ksourcetypical range for portland cement concrete (aggregate dependent)
100 mm part over a 50 °C swing118µm growth50µm growth2.36x less
Specific heat901J/kg·Ksourcebase material: commercially pure aluminium EN AW-1050A (Hydro), 20 °C900J/kg·Ksourcetypical (NIST guidance for thermal analysis)
Heats up and cools (diffusivity)90.9mm²/s211x faster0.431mm²/s
Thermal shock resistancenot sourcednot sourced
Melting point640–655°Csourcemelting rangenot sourced
Max service temperaturenot sourced65°Csourcecode long-term temperature limit (ASME Code, concrete containments)
Values for1100-O (annealed) commercially pure aluminium, Kaiser Aluminum Tube & Pipe Alloy 1100 Technical Data (Rev. 05/06), typical properties; specific heat from Hydro EN AW-1050A (99.5% Al) extruded-products datasheet (10/2018).Normal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC review

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Which is lighter, Aluminum 1100-O or Concrete?

Concrete is lighter: 2,320 kg/m³ against 2,710 kg/m³ for Aluminum 1100-O.

Which conducts heat better, Aluminum 1100-O or Concrete?

Aluminum 1100-O conducts heat better: 222 W/m·K against 0.9 W/m·K for Concrete.

Which expands less with temperature?

Concrete expands less: 10 µm/m·K against 23.6 µm/m·K for Aluminum 1100-O.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-O
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 1100-O
Strength against density

Related comparisons