Materials / Compare

Plastic ABS (bulk/injection) vs. Drywall

Compare Plastic ABS (bulk/injection) vs. Drywall strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS (bulk/injection)Bulk polymer (molded or machined)
DrywallNatural
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength45MPasourcetypical, tensile stress at yield 23 °Cnot given (tensile used)
Ultimate tensile strengthnot sourced1–2MPasourceambient range reported in review (Australian studies)
Compressive strengthnot sourced2.4MPasourcetypical, 70 F / 50% RH
Flexural strength65MPasourcetypical, 23 °Cnot sourced
Elongation at break10%sourcenominal strain at break, 23 °Cnot sourced
Young's modulus (stiffness)2.3GPasourcetypical1–2GPasourceambient range reported in review (Australian studies)
Density1,040kg/m³sourcetypicalnot sourced
Strength to weight43.3kN·m/kgnot sourced
Stiffness to weight2.21MN·m/kgnot sourced
Poisson's ratio0.39sourcetypical, ABS family (Covestro Part and Mold Design guide, Table 3-1)not sourced
Shear modulus0.827GPanot sourced
Bulk modulus3.48GPanot sourced
Speed of sound1,487m/snot sourced
Thermal
Thermal conductivity0.17W/m·Ksourcetypicalnot sourced
Thermal expansion80–110µm/m·Ksourcerange16.7µm/m·Ksourcetypical, unrestrained, 3.3-32 C
100 mm part over a 50 °C swing475µm growth83.5µm growth5.69x less
Specific heatnot sourced1,090J/kg·Ksourcetypical (from ASHRAE Handbook of Fundamentals, per GA)
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistance21.4W/mnot sourced
Max service temperature94°CsourceHDT 1.8 MPa (annealed 4 h/80 °C)52°Csourcemanufacturer sustained-exposure limit
Values forINEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittal

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic ABS (bulk/injection) stronger than Drywall?

Plastic ABS (bulk/injection) is stronger: its yield strength is 45 MPa against tensile strength 1.5 MPa for Drywall (30x).

Which is stiffer, Plastic ABS (bulk/injection) or Drywall?

Plastic ABS (bulk/injection) is stiffer: Young's modulus 2.3 GPa against 1.5 GPa for Drywall, so the same part in Plastic ABS (bulk/injection) deflects less under the same load.

Which expands less with temperature?

Drywall expands less: 16.7 µm/m·K against 95 µm/m·K for Plastic ABS (bulk/injection).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABS (bulk/injection)
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABS (bulk/injection)
Strength against density

Related comparisons