Compare Brick vs. Drywall strength, stiffness, weight and thermal properties.

Change either side
BrickNatural
DrywallNatural
Try it on a partA panel to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength5.1MPasourcemodulus of rupture (no direct tensile value)1–2MPasourceambient range reported in review (Australian studies)
Compressive strength77.9MPasourcemean unit compressive strength, solid extruded brick (survey mean; SD 30.8 MPa)2.4MPasourcetypical, 70 F / 50% RH
Elongation at breaknot sourcednot sourced
Young's modulus (stiffness)not sourced1–2GPasourceambient range reported in review (Australian studies)
Density2,082kg/m³sourceface brick density row used for k (BIA notes most fired clay brick 120-130 lb/ft3)not sourced
Strength to weight2.45kN·m/kgnot sourced
Stiffness to weightnot sourcednot sourced
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourcednot sourced
Thermal
Thermal conductivity0.92–1.12W/m·Ksourcerange for 130 lb/ft3 face brick (ASHRAE 2013 via BIA)not sourced
Thermal expansion7.2µm/m·KsourceTMS Code average coefficient, clay/shale unit masonry16.7µm/m·Ksourcetypical, unrestrained, 3.3-32 C
100 mm part over a 50 °C swing36µm growth2.32x less83.5µm growth
Specific heat837J/kg·Ksourcevalue used in BIA heat-capacity sample calculation1,090J/kg·Ksourcetypical (from ASHRAE Handbook of Fundamentals, per GA)
Heats up and cools (diffusivity)0.585mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Max service temperaturenot sourced52°Csourcemanufacturer sustained-exposure limit
Values forSolid extruded clay/shale brick units (BIA 1993 manufacturer survey, TN 3A 2024); face brick of 130 lb/ft3 for thermal properties (BIA TN 4, from ASHRAE 2013); CTE is the TMS Code value for clay/shale masonry1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittal

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Brick stronger than Drywall?

Brick is stronger: its tensile strength is 5.1 MPa against 1.5 MPa for Drywall (3.4x).

Which expands less with temperature?

Brick expands less: 7.2 µm/m·K against 16.7 µm/m·K for Drywall.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brick
Strength against density