Materials / Compare

Brick vs. SLA Resin Elastic 50A

Compare Brick vs. SLA Resin Elastic 50A strength, stiffness, weight and thermal properties.

Change either side
BrickNatural
SLA Resin Elastic 50A3D printed (SLA resin)
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength5.1MPasourcemodulus of rupture (no direct tensile value)3.4MPasourcetypical
Compressive strength77.9MPasourcemean unit compressive strength, solid extruded brick (survey mean; SD 30.8 MPa)not sourced
Elongation at breaknot sourced160%sourcetypical
Young's modulus (stiffness)not sourcednot sourced
Density2,082kg/m³sourceface brick density row used for k (BIA notes most fired clay brick 120-130 lb/ft3)1,010kg/m³sourcetypical
Strength to weight2.45kN·m/kg3.37kN·m/kg37% higher
Stiffness to weightnot sourcednot sourced
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourcednot sourced
Thermal
Thermal conductivity0.92–1.12W/m·Ksourcerange for 130 lb/ft3 face brick (ASHRAE 2013 via BIA)not sourced
Thermal expansion7.2µm/m·KsourceTMS Code average coefficient, clay/shale unit masonrynot sourced
100 mm part over a 50 °C swing36µm growthnot sourced
Specific heat837J/kg·Ksourcevalue used in BIA heat-capacity sample calculationnot sourced
Heats up and cools (diffusivity)0.585mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Glass transitionnot sourced-34.5°CsourceDMA
Values forSolid extruded clay/shale brick units (BIA 1993 manufacturer survey, TN 3A 2024); face brick of 130 lb/ft3 for thermal properties (BIA TN 4, from ASHRAE 2013); CTE is the TMS Code value for clay/shale masonryFormlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Brick stronger than SLA Resin Elastic 50A?

Brick is stronger: its tensile strength is 5.1 MPa against 3.4 MPa for SLA Resin Elastic 50A (1.5x).

Which is lighter, Brick or SLA Resin Elastic 50A?

SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 2,082 kg/m³ for Brick.

Which is lighter for the same job, Brick or SLA Resin Elastic 50A?

For the same stiffness or strength: SLA Resin Elastic 50A is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beBrickSLA Resin Elastic 50A
Strong rod or tie37% heavierlighter
Strong beam1.57x heavierlighter
Strong panel or plate1.68x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30BrickSLA Resin Elastic 50A
Strength against density

Related comparisons