Materials / Compare

Plastic PTFE vs. SLA Resin Elastic 50A

Compare Plastic PTFE vs. SLA Resin Elastic 50A strength, stiffness, weight and thermal properties.

Change either side
Plastic PTFEBulk polymer (molded or machined)
SLA Resin Elastic 50A3D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength9MPasourcetypical yield strength at 23 °C (Teflon PTFE, Table 8)not given (tensile used)
Ultimate tensile strength39.3MPasourcetypical, skived tape 0.13 mm3.4MPasourcetypical
Elongation at break350%sourcetypical, skived tape 0.13 mm160%sourcetypical
Young's modulus (stiffness)not sourcednot sourced
Density2,160kg/m³sourcetypical (standard specific gravity, ASTM D4894)1,010kg/m³sourcetypical
Strength to weight4.17kN·m/kg24% higher3.37kN·m/kg
Stiffness to weightnot sourcednot sourced
Poisson's ratio0.46sourcetypical, 23 °C (Teflon PTFE resins, Chemours handbook)not sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourcednot sourced
Thermal
Thermal conductivity0.25W/m·Ksourcetypical, granular resin, 4.6 mm specimennot sourced
Thermal expansion100µm/m·Ksourcetypical, granular resin, 23-60 °C (ASTM E228)not sourced
100 mm part over a 50 °C swing500µm growthnot sourced
Specific heat1,400J/kg·Ksourcetypical, granular resin, 20 °C (ASTM D4591)not sourced
Heats up and cools (diffusivity)0.0827mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Melting point327°Csourcesecond melting peak (sintered polymer), +/-10not sourced
Glass transitionnot sourced-34.5°CsourceDMA
Max service temperature260°Csourceservice temperature (Chemours general Teflon PTFE statement)not sourced
Values forChemours Teflon PTFE 7C X granular molding resin, typical values (tensile/elongation measured on 0.13 mm skived tape)Formlabs Elastic 50A Resin V2 (FLELCL02), TDS Rev. 01 24.01.2024; parts printed on Form 3, 100 µm, Elastic 50A V2 settings and post-processing; tensile on Die C specimens cut from printed sheets after 3+ h at 23 °C.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Elastic 50A is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic PTFE stronger than SLA Resin Elastic 50A?

Plastic PTFE is stronger: its yield strength is 9 MPa against tensile strength 3.4 MPa for SLA Resin Elastic 50A (2.65x).

Which is lighter, Plastic PTFE or SLA Resin Elastic 50A?

SLA Resin Elastic 50A is lighter: 1,010 kg/m³ against 2,160 kg/m³ for Plastic PTFE.

Which is lighter for the same job, Plastic PTFE or SLA Resin Elastic 50A?

For the same stiffness or strength: Plastic PTFE is lighter for a strong rod or tie; SLA Resin Elastic 50A is lighter for a strong beam, strong panel or plate.

Part that must bePlastic PTFESLA Resin Elastic 50A
Strong rod or tielighter24% heavier
Strong beam12% heavierlighter
Strong panel or plate31% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PTFESLA Resin Elastic 50A
Strength against density

Related comparisons