Materials / Plastic

Plastic PTFE

Plastic PTFE (Teflon) strength, stiffness, density and thermal properties, with their source.

A bracket in Plastic PTFE, smooth finish.

ProcessBulk polymer (molded or machined)
Mechanical
Yield strength9MPasourcetypical yield strength at 23 °C (Teflon PTFE, Table 8)
Ultimate tensile strength39.3MPasourcetypical, skived tape 0.13 mm
Elongation at break350%sourcetypical, skived tape 0.13 mm
Young's modulus (stiffness)not sourced
Density2,160kg/m³sourcetypical (standard specific gravity, ASTM D4894)
Strength to weight4.17kN·m/kg
Stiffness to weightnot sourced
Poisson's ratio0.46sourcetypical, 23 °C (Teflon PTFE resins, Chemours handbook)
Shear modulusnot sourced
Bulk modulusnot sourced
Speed of soundnot sourced
Thermal
Thermal conductivity0.25W/m·Ksourcetypical, granular resin, 4.6 mm specimen
Thermal expansion100µm/m·Ksourcetypical, granular resin, 23-60 °C (ASTM E228)
100 mm part over a 50 °C swing500µm growth
Specific heat1,400J/kg·Ksourcetypical, granular resin, 20 °C (ASTM D4591)
Heats up and cools (diffusivity)0.0827mm²/s
Thermal shock resistancenot sourced
Melting point327°Csourcesecond melting peak (sintered polymer), +/-10
Max service temperature260°Csourceservice temperature (Chemours general Teflon PTFE statement)
Values forChemours Teflon PTFE 7C X granular molding resin, typical values (tensile/elongation measured on 0.13 mm skived tape)

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless Steel
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PTFE
Strength against density

Compare Plastic PTFE with