Materials / Compare

Plastic Nylon PA66 vs. Plastic PTFE

Compare Plastic Nylon PA66 vs. Plastic PTFE strength, stiffness, weight and thermal properties.

Change either side
Plastic Nylon PA66Bulk polymer (molded or machined)
Plastic PTFEBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength85MPasourcetypical, dry9MPasourcetypical yield strength at 23 °C (Teflon PTFE, Table 8)
Ultimate tensile strengthnot sourced39.3MPasourcetypical, skived tape 0.13 mm
Elongation at break30%sourcenominal strain at break, dry350%sourcetypical, skived tape 0.13 mm
Young's modulus (stiffness)3GPasourcetypical, drynot sourced
Density1,130kg/m³sourcetypical2,160kg/m³sourcetypical (standard specific gravity, ASTM D4894)
Strength to weight75.2kN·m/kg18.1x higher4.17kN·m/kg
Stiffness to weight2.65MN·m/kgnot sourced
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)0.46sourcetypical, 23 °C (Teflon PTFE resins, Chemours handbook)
Shear modulus1.07GPanot sourced
Bulk modulus5GPanot sourced
Speed of sound1,629m/snot sourced
Thermal
Thermal conductivity0.33W/m·Ksourcetypical0.25W/m·Ksourcetypical, granular resin, 4.6 mm specimen
Thermal expansion98µm/m·Ksourcelongitudinal, 23-55 °C100µm/m·Ksourcetypical, granular resin, 23-60 °C (ASTM E228)
100 mm part over a 50 °C swing490µm growth2% less500µm growth
Specific heat1,700J/kg·Ksourcetypical1,400J/kg·Ksourcetypical, granular resin, 20 °C (ASTM D4591)
Heats up and cools (diffusivity)0.172mm²/s2.08x faster0.0827mm²/s
Thermal shock resistance57.2W/mnot sourced
Melting point260°CsourceDSC327°Csourcesecond melting peak (sintered polymer), +/-10
Max service temperature101°CsourceIEC 60216 temperature index, 20000 h260°Csourceservice temperature (Chemours general Teflon PTFE statement)
Values forBASF Ultramid A3K (PA66, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)Chemours Teflon PTFE 7C X granular molding resin, typical values (tensile/elongation measured on 0.13 mm skived tape)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic Nylon PA66 stronger than Plastic PTFE?

Plastic Nylon PA66 is stronger: its yield strength is 85 MPa against 9 MPa for Plastic PTFE (9.44x).

Which is lighter, Plastic Nylon PA66 or Plastic PTFE?

Plastic Nylon PA66 is lighter: 1,130 kg/m³ against 2,160 kg/m³ for Plastic PTFE.

Which is lighter for the same job, Plastic Nylon PA66 or Plastic PTFE?

For the same stiffness or strength: Plastic Nylon PA66 is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic Nylon PA66Plastic PTFE
Strong rod or tielighter18.1x heavier
Strong beamlighter8.54x heavier
Strong panel or platelighter5.87x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Nylon PA66 or Plastic PTFE?

Plastic Nylon PA66 conducts heat better: 0.33 W/m·K against 0.25 W/m·K for Plastic PTFE.

Which expands less with temperature?

Plastic Nylon PA66 expands less: 98 µm/m·K against 100 µm/m·K for Plastic PTFE.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Nylon PA66
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Nylon PA66Plastic PTFE
Strength against density

Related comparisons