Materials / Plastic

Plastic Nylon PA66

Plastic Nylon PA66 (dry) strength, stiffness, density and thermal properties, with their source.

A bracket in Plastic Nylon PA66, smooth finish.

ProcessBulk polymer (molded or machined)
Mechanical
Yield strength85MPasourcetypical, dry
Ultimate tensile strengthnot sourced
Elongation at break30%sourcenominal strain at break, dry
Young's modulus (stiffness)3GPasourcetypical, dry
Density1,130kg/m³sourcetypical
Strength to weight75.2kN·m/kg
Stiffness to weight2.65MN·m/kg
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
Shear modulus1.07GPa
Bulk modulus5GPa
Speed of sound1,629m/s
Thermal
Thermal conductivity0.33W/m·Ksourcetypical
Thermal expansion98µm/m·Ksourcelongitudinal, 23-55 °C
100 mm part over a 50 °C swing490µm growth
Specific heat1,700J/kg·Ksourcetypical
Heats up and cools (diffusivity)0.172mm²/s
Thermal shock resistance57.2W/m
Melting point260°CsourceDSC
Max service temperature101°CsourceIEC 60216 temperature index, 20000 h
Values forBASF Ultramid A3K (PA66, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Nylon PA66
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Nylon PA66
Strength against density

Compare Plastic Nylon PA66 with