Mechanical
Yield strength45MPasourcetypical, tensile stress at yield 23 °C85MPasourcetypical, dry
Ultimate tensile strengthnot sourcednot sourced
Flexural strength65MPasourcetypical, 23 °Cnot sourced
Elongation at break10%sourcenominal strain at break, 23 °C30%sourcenominal strain at break, dry
Young's modulus (stiffness)2.3GPasourcetypical3GPasourcetypical, dry
Density1,040kg/m³sourcetypical1,130kg/m³sourcetypical
Strength to weight43.3kN·m/kg75.2kN·m/kg1.74x higher
Stiffness to weight2.21MN·m/kg2.65MN·m/kg20% higher
Poisson's ratio0.39sourcetypical, ABS family (Covestro Part and Mold Design guide, Table 3-1)0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
Shear modulus0.827GPa1.07GPa30% stiffer in shear
Bulk modulus3.48GPa5GPa
Speed of sound1,487m/s1,629m/s
Thermal
Thermal conductivity0.17W/m·Ksourcetypical0.33W/m·Ksourcetypical1.94x more heat through a fin
Thermal expansion80–110µm/m·Ksourcerange98µm/m·Ksourcelongitudinal, 23-55 °C
100 mm part over a 50 °C swing475µm growth3% less490µm growth
Specific heatnot sourced1,700J/kg·Ksourcetypical
Heats up and cools (diffusivity)not sourced0.172mm²/s
Thermal shock resistance21.4W/m57.2W/m2.68x more resistant
Melting pointnot sourced260°CsourceDSC
Max service temperature94°CsourceHDT 1.8 MPa (annealed 4 h/80 °C)101°CsourceIEC 60216 temperature index, 20000 h
Values forINEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)BASF Ultramid A3K (PA66, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic ABS (bulk/injection) stronger than Plastic Nylon PA66?

Plastic Nylon PA66 is stronger: its yield strength is 85 MPa against 45 MPa for Plastic ABS (bulk/injection) (1.89x).

Which is lighter, Plastic ABS (bulk/injection) or Plastic Nylon PA66?

Plastic ABS (bulk/injection) is lighter: 1,040 kg/m³ against 1,130 kg/m³ for Plastic Nylon PA66.

Which is stiffer, Plastic ABS (bulk/injection) or Plastic Nylon PA66?

Plastic Nylon PA66 is stiffer: Young's modulus 3 GPa against 2.3 GPa for Plastic ABS (bulk/injection), so the same part in Plastic Nylon PA66 deflects less under the same load.

Which is lighter for the same job, Plastic ABS (bulk/injection) or Plastic Nylon PA66?

For the same stiffness or strength: Plastic Nylon PA66 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABS (bulk/injection)Plastic Nylon PA66
Stiff rod or tie (tension)20% heavierlighter
Stiff beam (bending)5% heavierlighter
Stiff panel or plateabout equalabout equal
Strong rod or tie1.74x heavierlighter
Strong beam41% heavierlighter
Strong panel or plate26% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic ABS (bulk/injection) or Plastic Nylon PA66?

Plastic Nylon PA66 conducts heat better: 0.33 W/m·K against 0.17 W/m·K for Plastic ABS (bulk/injection).

Which expands less with temperature?

Plastic ABS (bulk/injection) expands less: 95 µm/m·K against 98 µm/m·K for Plastic Nylon PA66.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABS (bulk/injection)Plastic Nylon PA66
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABS (bulk/injection)Plastic Nylon PA66
Strength against density

Related comparisons