Materials / Compare

Plastic Nylon PA66 vs. SLA Resin Tough 2000

Compare Plastic Nylon PA66 vs. SLA Resin Tough 2000 strength, stiffness, weight and thermal properties.

Change either side
Plastic Nylon PA66Bulk polymer (molded or machined)
SLA Resin Tough 20003D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength85MPasourcetypical, dry40.4MPasourcetypical
Ultimate tensile strengthnot sourced40.4MPasourcetypical
Flexural strengthnot sourced67MPasourcetypical
Elongation at break30%sourcenominal strain at break, dry79%sourcetypical
Young's modulus (stiffness)3GPasourcetypical, dry1.8GPasourcetypical
Density1,130kg/m³sourcetypical1,090kg/m³sourcetypical
Strength to weight75.2kN·m/kg2.03x higher37.1kN·m/kg
Stiffness to weight2.65MN·m/kg1.61x higher1.65MN·m/kg
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)not sourced
Shear modulus1.07GPanot sourced
Bulk modulus5GPanot sourced
Speed of sound1,629m/s1,285m/s
Thermal
Thermal conductivity0.33W/m·Ksourcetypicalnot sourced
Thermal expansion98µm/m·Ksourcelongitudinal, 23-55 °C134µm/m·Ksourcemean 0-150 °C
100 mm part over a 50 °C swing490µm growth37% less671µm growth
Specific heat1,700J/kg·Ksourcetypicalnot sourced
Heats up and cools (diffusivity)0.172mm²/snot sourced
Thermal shock resistance57.2W/mnot sourced
Melting point260°CsourceDSCnot sourced
Glass transitionnot sourced112°CsourceDMA
Max service temperature101°CsourceIEC 60216 temperature index, 20000 h57°CsourceHDT 1.8 MPa
Values forBASF Ultramid A3K (PA66, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic Nylon PA66 stronger than SLA Resin Tough 2000?

Plastic Nylon PA66 is stronger: its yield strength is 85 MPa against 40.4 MPa for SLA Resin Tough 2000 (2.1x).

Which is lighter, Plastic Nylon PA66 or SLA Resin Tough 2000?

SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 1,130 kg/m³ for Plastic Nylon PA66.

Which is stiffer, Plastic Nylon PA66 or SLA Resin Tough 2000?

Plastic Nylon PA66 is stiffer: Young's modulus 3 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Plastic Nylon PA66 deflects less under the same load.

Which is lighter for the same job, Plastic Nylon PA66 or SLA Resin Tough 2000?

For the same stiffness or strength: Plastic Nylon PA66 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic Nylon PA66SLA Resin Tough 2000
Stiff rod or tie (tension)lighter1.61x heavier
Stiff beam (bending)lighter25% heavier
Stiff panel or platelighter14% heavier
Strong rod or tielighter2.03x heavier
Strong beamlighter1.58x heavier
Strong panel or platelighter40% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which expands less with temperature?

Plastic Nylon PA66 expands less: 98 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Nylon PA66SLA Resin Tough 2000
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Nylon PA66SLA Resin Tough 2000
Strength against density

Related comparisons