Materials / Compare

Plastic ABS (bulk/injection) vs. SLA Resin Tough 2000

Compare Plastic ABS (bulk/injection) vs. SLA Resin Tough 2000 strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS (bulk/injection)Bulk polymer (molded or machined)
SLA Resin Tough 20003D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength45MPasourcetypical, tensile stress at yield 23 °C40.4MPasourcetypical
Ultimate tensile strengthnot sourced40.4MPasourcetypical
Flexural strength65MPasourcetypical, 23 °C67MPasourcetypical
Elongation at break10%sourcenominal strain at break, 23 °C79%sourcetypical
Young's modulus (stiffness)2.3GPasourcetypical28% stiffer1.8GPasourcetypical
Density1,040kg/m³sourcetypical1,090kg/m³sourcetypical
Strength to weight43.3kN·m/kg17% higher37.1kN·m/kg
Stiffness to weight2.21MN·m/kg34% higher1.65MN·m/kg
Poisson's ratio0.39sourcetypical, ABS family (Covestro Part and Mold Design guide, Table 3-1)not sourced
Shear modulus0.827GPanot sourced
Bulk modulus3.48GPanot sourced
Speed of sound1,487m/s1,285m/s
Thermal
Thermal conductivity0.17W/m·Ksourcetypicalnot sourced
Thermal expansion80–110µm/m·Ksourcerange134µm/m·Ksourcemean 0-150 °C
100 mm part over a 50 °C swing475µm growth41% less671µm growth
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistance21.4W/mnot sourced
Glass transitionnot sourced112°CsourceDMA
Max service temperature94°CsourceHDT 1.8 MPa (annealed 4 h/80 °C)57°CsourceHDT 1.8 MPa
Values forINEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS (bulk/injection) stronger than SLA Resin Tough 2000?

Plastic ABS (bulk/injection) is stronger: its yield strength is 45 MPa against 40.4 MPa for SLA Resin Tough 2000 (11%).

Which is lighter, Plastic ABS (bulk/injection) or SLA Resin Tough 2000?

Plastic ABS (bulk/injection) is lighter: 1,040 kg/m³ against 1,090 kg/m³ for SLA Resin Tough 2000.

Which is stiffer, Plastic ABS (bulk/injection) or SLA Resin Tough 2000?

Plastic ABS (bulk/injection) is stiffer: Young's modulus 2.3 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Plastic ABS (bulk/injection) deflects less under the same load.

Which is lighter for the same job, Plastic ABS (bulk/injection) or SLA Resin Tough 2000?

For the same stiffness or strength: Plastic ABS (bulk/injection) is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABS (bulk/injection)SLA Resin Tough 2000
Stiff rod or tie (tension)lighter34% heavier
Stiff beam (bending)lighter18% heavier
Stiff panel or platelighter14% heavier
Strong rod or tielighter17% heavier
Strong beamlighter13% heavier
Strong panel or platelighter11% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which expands less with temperature?

Plastic ABS (bulk/injection) expands less: 95 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABS (bulk/injection)SLA Resin Tough 2000
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABS (bulk/injection)SLA Resin Tough 2000
Strength against density