Materials / Compare

Plastic PETG vs. Plastic PTFE

Compare Plastic PETG vs. Plastic PTFE strength, stiffness, weight and thermal properties.

Change either side
Plastic PETG3D printed (FDM)
Plastic PTFEBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength46.2MPasourcetypical9MPasourcetypical yield strength at 23 °C (Teflon PTFE, Table 8)
Ultimate tensile strength46.2MPasourcetypical, peak stress (= stress at yield)39.3MPasourcetypical, skived tape 0.13 mm
Flexural strength78.9MPasourcetypicalnot sourced
Elongation at break7.6%sourcetypical350%sourcetypical, skived tape 0.13 mm
Young's modulus (stiffness)1.94GPasourcetypicalnot sourced
Density1,270kg/m³sourcetypical2,160kg/m³sourcetypical (standard specific gravity, ASTM D4894)
Strength to weight36.4kN·m/kg8.73x higher4.17kN·m/kg
Stiffness to weight1.53MN·m/kgnot sourced
Poisson's rationot sourced0.46sourcetypical, 23 °C (Teflon PTFE resins, Chemours handbook)
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,236m/snot sourced
Thermal
Thermal conductivity0.21W/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical0.25W/m·Ksourcetypical, granular resin, 4.6 mm specimen
Thermal expansion51µm/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical100µm/m·Ksourcetypical, granular resin, 23-60 °C (ASTM E228)
100 mm part over a 50 °C swing255µm growth1.96x less500µm growth
Specific heat1,300J/kg·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)1,400J/kg·Ksourcetypical, granular resin, 20 °C (ASTM D4591)
Heats up and cools (diffusivity)0.127mm²/s1.54x faster0.0827mm²/s
Thermal shock resistancenot sourcednot sourced
Melting pointnot sourced327°Csourcesecond melting peak (sintered polymer), +/-10
Glass transition77.4°Csourcetypicalnot sourced
Max service temperature76.2°CsourceHDT 0.455 MPa (printed specimens)260°Csourceservice temperature (Chemours general Teflon PTFE statement)
Values forUltimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022.Chemours Teflon PTFE 7C X granular molding resin, typical values (tensile/elongation measured on 0.13 mm skived tape)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic PETG stronger than Plastic PTFE?

Plastic PETG is stronger: its yield strength is 46.2 MPa against 9 MPa for Plastic PTFE (5.13x).

Which is lighter, Plastic PETG or Plastic PTFE?

Plastic PETG is lighter: 1,270 kg/m³ against 2,160 kg/m³ for Plastic PTFE.

Which is lighter for the same job, Plastic PETG or Plastic PTFE?

For the same stiffness or strength: Plastic PETG is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PETGPlastic PTFE
Strong rod or tielighter8.73x heavier
Strong beamlighter5.06x heavier
Strong panel or platelighter3.85x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic PETG or Plastic PTFE?

Plastic PTFE conducts heat better: 0.25 W/m·K against 0.21 W/m·K for Plastic PETG.

Which expands less with temperature?

Plastic PETG expands less: 51 µm/m·K against 100 µm/m·K for Plastic PTFE.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PETG
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PETGPlastic PTFE
Strength against density

Related comparisons