Materials / Compare

FDM Polycarbonate vs. Plastic PETG

Compare FDM Polycarbonate vs. Plastic PETG strength, stiffness, weight and thermal properties.

Change either side
FDM Polycarbonate3D printed (FDM)
Plastic PETG3D printed (FDM)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength53.3MPasourcetypical15% stronger46.2MPasourcetypical
Ultimate tensile strength53.3MPasourcetypical, peak stress (= stress at yield)15% stronger46.2MPasourcetypical, peak stress (= stress at yield)
Flexural strength89.4MPasourcetypical13% stronger in bending78.9MPasourcetypical
Elongation at break9.2%sourcetypical21% more ductile7.6%sourcetypical
Young's modulus (stiffness)2.39GPasourcetypical23% stiffer1.94GPasourcetypical
Density1,180–1,200kg/m³sourcerange1,270kg/m³sourcetypical
Strength to weight44.8kN·m/kg23% higher36.4kN·m/kg
Stiffness to weight2.01MN·m/kg32% higher1.53MN·m/kg
Poisson's ratio0.38sourcebase material: polycarbonate family typical (Covestro Part and Mold Design guide, Table 3-1)not sourced
Shear modulus0.867GPanot sourced
Bulk modulus3.33GPanot sourced
Speed of sound1,418m/s1,236m/s
Thermal
Thermal conductivity0.2W/m·Ksourcebase material: Covestro Makrolon 2405 injection-molding PC, typical, through-plane, 23 °C0.21W/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical
Thermal expansion65µm/m·Ksourcebase material: Covestro Makrolon 2405 injection-molding PC, typical, 23-55 °C, parallel51µm/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical
100 mm part over a 50 °C swing325µm growth255µm growth27% less
Specific heatnot sourced1,300J/kg·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)
Heats up and cools (diffusivity)not sourced0.127mm²/s
Thermal shock resistance42.5W/mnot sourced
Glass transition108°Csourcetypical77.4°Csourcetypical
Max service temperature105°CsourceHDT 0.455 MPa (printed specimens)37% hotter76.2°CsourceHDT 0.455 MPa (printed specimens)
Values forUltimaker PC, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 20, 2022.Ultimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM Polycarbonate and Plastic PETG are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is FDM Polycarbonate stronger than Plastic PETG?

FDM Polycarbonate is stronger: its yield strength is 53.3 MPa against 46.2 MPa for Plastic PETG (15%).

Which is lighter, FDM Polycarbonate or Plastic PETG?

FDM Polycarbonate is lighter: 1,190 kg/m³ against 1,270 kg/m³ for Plastic PETG.

Which is stiffer, FDM Polycarbonate or Plastic PETG?

FDM Polycarbonate is stiffer: Young's modulus 2.39 GPa against 1.94 GPa for Plastic PETG, so the same part in FDM Polycarbonate deflects less under the same load.

Which is lighter for the same job, FDM Polycarbonate or Plastic PETG?

For the same stiffness or strength: FDM Polycarbonate is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM PolycarbonatePlastic PETG
Stiff rod or tie (tension)lighter32% heavier
Stiff beam (bending)lighter19% heavier
Stiff panel or platelighter14% heavier
Strong rod or tielighter23% heavier
Strong beamlighter17% heavier
Strong panel or platelighter15% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, FDM Polycarbonate or Plastic PETG?

FDM Polycarbonate stretches further before it breaks: 9.2% elongation at break against 7.6% for Plastic PETG.

Which handles higher temperatures, FDM Polycarbonate or Plastic PETG?

FDM Polycarbonate does: 105 °C against 76.2 °C for Plastic PETG, both HDT 0.455 MPa (printed specimens).

Which conducts heat better, FDM Polycarbonate or Plastic PETG?

Plastic PETG conducts heat better: 0.21 W/m·K against 0.2 W/m·K for FDM Polycarbonate.

Which expands less with temperature?

Plastic PETG expands less: 51 µm/m·K against 65 µm/m·K for FDM Polycarbonate.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelFDM PolycarbonatePlastic PETG
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickFDM PolycarbonatePlastic PETG
Strength against density