Materials / Compare

FDM Polycarbonate vs. SLA Resin Standard

Compare FDM Polycarbonate vs. SLA Resin Standard strength, stiffness, weight and thermal properties.

Change either side
FDM Polycarbonate3D printed (FDM)
SLA Resin Standard3D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength53.3MPasourcetypicalnot given (tensile used)
Ultimate tensile strength53.3MPasourcetypical, peak stress (= stress at yield)60MPasourcetypical
Flexural strength89.4MPasourcetypical105MPasourcetypical17% stronger in bending
Elongation at break9.2%sourcetypical15% more ductile8%sourcetypical
Young's modulus (stiffness)2.39GPasourcetypical2.75GPasourcetypical15% stiffer
Density1,180–1,200kg/m³sourcerangenot sourced
Strength to weight44.8kN·m/kgnot sourced
Stiffness to weight2.01MN·m/kgnot sourced
Poisson's ratio0.38sourcebase material: polycarbonate family typical (Covestro Part and Mold Design guide, Table 3-1)not sourced
Shear modulus0.867GPanot sourced
Bulk modulus3.33GPanot sourced
Speed of sound1,418m/snot sourced
Thermal
Thermal conductivity0.2W/m·Ksourcebase material: Covestro Makrolon 2405 injection-molding PC, typical, through-plane, 23 °Cnot sourced
Thermal expansion65µm/m·Ksourcebase material: Covestro Makrolon 2405 injection-molding PC, typical, 23-55 °C, parallelnot sourced
100 mm part over a 50 °C swing325µm growthnot sourced
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistance42.5W/mnot sourced
Glass transition108°Csourcetypicalnot sourced
Max service temperature105°CsourceHDT 0.455 MPa (printed specimens)59°CsourceHDT 1.8 MPa
Values forUltimaker PC, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 20, 2022.Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM Polycarbonate and SLA Resin Standard are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is FDM Polycarbonate stronger than SLA Resin Standard?

SLA Resin Standard is stronger: its tensile strength is 60 MPa against yield strength 53.3 MPa for FDM Polycarbonate (13%).

Which is stiffer, FDM Polycarbonate or SLA Resin Standard?

SLA Resin Standard is stiffer: Young's modulus 2.75 GPa against 2.39 GPa for FDM Polycarbonate, so the same part in SLA Resin Standard deflects less under the same load.

Which is more ductile, FDM Polycarbonate or SLA Resin Standard?

FDM Polycarbonate stretches further before it breaks: 9.2% elongation at break against 8% for SLA Resin Standard.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM Polycarbonate
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM Polycarbonate
Strength against density