Materials / Compare

Plastic Nylon vs. SLA Resin Standard

Compare Plastic Nylon vs. SLA Resin Standard strength, stiffness, weight and thermal properties.

Change either side
Plastic Nylon3D printed (FDM)
SLA Resin Standard3D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength63.1MPasourcetypicalnot given (tensile used)
Ultimate tensile strength63.1MPasourcetypical, peak stress (= stress at yield)60MPasourcetypical
Flexural strength82.9MPasourcetypical105MPasourcetypical27% stronger in bending
Elongation at breaknot sourced8%sourcetypical
Young's modulus (stiffness)2.33GPasourcetypical2.75GPasourcetypical18% stiffer
Density1,140kg/m³sourcetypicalnot sourced
Strength to weight55.4kN·m/kgnot sourced
Stiffness to weight2.04MN·m/kgnot sourced
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)not sourced
Shear modulus0.833GPanot sourced
Bulk modulus3.89GPanot sourced
Speed of sound1,430m/snot sourced
Thermal
Thermal conductivity0.33W/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)not sourced
Thermal expansion98–102µm/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 Cnot sourced
100 mm part over a 50 °C swing500µm growthnot sourced
Specific heat1,700J/kg·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)not sourced
Heats up and cools (diffusivity)0.17mm²/snot sourced
Thermal shock resistance53.6W/mnot sourced
Melting point188°Csourcetypicalnot sourced
Glass transition55.1°Csourcetypicalnot sourced
Max service temperature89.2°CsourceHDT 0.455 MPa (printed specimens)59°CsourceHDT 1.8 MPa
Values forUltimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic Nylon and SLA Resin Standard are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic Nylon stronger than SLA Resin Standard?

Plastic Nylon is stronger: its yield strength is 63.1 MPa against tensile strength 60 MPa for SLA Resin Standard (5%).

Which is stiffer, Plastic Nylon or SLA Resin Standard?

SLA Resin Standard is stiffer: Young's modulus 2.75 GPa against 2.33 GPa for Plastic Nylon, so the same part in SLA Resin Standard deflects less under the same load.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Nylon
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPURubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Nylon
Strength against density

Related comparisons