Materials / Compare

Plastic Nylon vs. Plastic POM/Acetal

Compare Plastic Nylon vs. Plastic POM/Acetal strength, stiffness, weight and thermal properties.

Change either side
Plastic Nylon3D printed (FDM)
Plastic POM/AcetalBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength63.1MPasourcetypical69MPasourcetypical (single ASTM D638 tensile strength)
Ultimate tensile strength63.1MPasourcetypical, peak stress (= stress at yield)69MPasourcetypical
Compressive strengthnot sourced124MPasourcecompressive stress at 10% deformation
Flexural strength82.9MPasourcetypical99MPasourceflexural yield strength, typical
Elongation at breaknot sourced75%sourcetypical
Young's modulus (stiffness)2.33GPasourcetypical2.8GPasourcetypical20% stiffer
Density1,140kg/m³sourcetypical1,420kg/m³sourcetypical (DuPont product information for Delrin 100 NC010; 'The data listed here fall within the normal range of product properties')
Strength to weight55.4kN·m/kg14% higher48.6kN·m/kg
Stiffness to weight2.04MN·m/kg4% higher1.97MN·m/kg
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)0.35sourcetypical
Shear modulus0.833GPa1.04GPa25% stiffer in shear
Bulk modulus3.89GPa3.11GPa
Speed of sound1,430m/s1,404m/s
Thermal
Thermal conductivity0.33W/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)0.4W/m·Ksourcetypical
Thermal expansion98–102µm/m·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 C122µm/m·Ksourcemean, 29 to 60 °C
100 mm part over a 50 °C swing500µm growth22% less610µm growth
Specific heat1,700J/kg·Ksourcebase material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)1,465J/kg·Ksourceaverage -18 to 100 °C, Delrin acetal resins (not grade-specific)
Heats up and cools (diffusivity)0.17mm²/s0.192mm²/s13% faster
Thermal shock resistance53.6W/m2% more resistant52.5W/m
Melting point188°Csourcetypical175°Csourcecrystalline melting point
Glass transition55.1°Csourcetypicalnot sourced
Max service temperature89.2°CsourceHDT 0.455 MPa (printed specimens)125°CsourceHDT 1.8 MPa (annealed)
Values forUltimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.DuPont Delrin 100 acetal homopolymer, Table 2 'Typical Properties of Delrin Acetal Resins' (ASTM methods), Delrin Design Guide Module III hosted on delrin.com

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic Nylon stronger than Plastic POM/Acetal?

Plastic POM/Acetal is stronger: its yield strength is 69 MPa against 63.1 MPa for Plastic Nylon (9%).

Which is lighter, Plastic Nylon or Plastic POM/Acetal?

Plastic Nylon is lighter: 1,140 kg/m³ against 1,420 kg/m³ for Plastic POM/Acetal.

Which is stiffer, Plastic Nylon or Plastic POM/Acetal?

Plastic POM/Acetal is stiffer: Young's modulus 2.8 GPa against 2.33 GPa for Plastic Nylon, so the same part in Plastic POM/Acetal deflects less under the same load.

Which is lighter for the same job, Plastic Nylon or Plastic POM/Acetal?

For the same stiffness or strength: Plastic Nylon is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic NylonPlastic POM/Acetal
Stiff rod or tie (tension)lighter4% heavier
Stiff beam (bending)lighter14% heavier
Stiff panel or platelighter17% heavier
Strong rod or tielighter14% heavier
Strong beamlighter17% heavier
Strong panel or platelighter19% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Nylon or Plastic POM/Acetal?

Plastic POM/Acetal conducts heat better: 0.4 W/m·K against 0.33 W/m·K for Plastic Nylon.

Which expands less with temperature?

Plastic Nylon expands less: 100 µm/m·K against 122 µm/m·K for Plastic POM/Acetal.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic NylonPlastic POM/Acetal
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPURubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic NylonPlastic POM/Acetal
Strength against density

Related comparisons