ProcessBulk polymer (molded or machined)
Mechanical
Yield strength69MPasourcetypical (single ASTM D638 tensile strength)
Ultimate tensile strength69MPasourcetypical
Compressive strength124MPasourcecompressive stress at 10% deformation
Flexural strength99MPasourceflexural yield strength, typical
Elongation at break75%sourcetypical
Young's modulus (stiffness)2.8GPasourcetypical
Density1,420kg/m³sourcetypical (DuPont product information for Delrin 100 NC010; 'The data listed here fall within the normal range of product properties')
Strength to weight48.6kN·m/kg
Stiffness to weight1.97MN·m/kg
Poisson's ratio0.35sourcetypical
Shear modulus1.04GPa
Bulk modulus3.11GPa
Speed of sound1,404m/s
Thermal
Thermal conductivity0.4W/m·Ksourcetypical
Thermal expansion122µm/m·Ksourcemean, 29 to 60 °C
100 mm part over a 50 °C swing610µm growth
Specific heat1,465J/kg·Ksourceaverage -18 to 100 °C, Delrin acetal resins (not grade-specific)
Heats up and cools (diffusivity)0.192mm²/s
Thermal shock resistance52.5W/m
Melting point175°Csourcecrystalline melting point
Max service temperature125°CsourceHDT 1.8 MPa (annealed)
Values forDuPont Delrin 100 acetal homopolymer, Table 2 'Typical Properties of Delrin Acetal Resins' (ASTM methods), Delrin Design Guide Module III hosted on delrin.com

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic POM/Acetal
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic POM/Acetal
Strength against density

Compare Plastic POM/Acetal with