Materials / Compare

Plastic POM/Acetal vs. Plastic TPU

Compare Plastic POM/Acetal vs. Plastic TPU strength, stiffness, weight and thermal properties.

Change either side
Plastic POM/AcetalBulk polymer (molded or machined)
Plastic TPU3D printed (FDM)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength69MPasourcetypical (single ASTM D638 tensile strength)not given (tensile used)
Ultimate tensile strength69MPasourcetypical23.7MPasourcetypical, stress at break
Compressive strength124MPasourcecompressive stress at 10% deformationnot sourced
Flexural strength99MPasourceflexural yield strength, typical4.1MPasourcetypical
Elongation at break75%sourcetypicalnot sourced
Young's modulus (stiffness)2.8GPasourcetypical41.8x stiffer0.067GPasourcetypical
Density1,420kg/m³sourcetypical (DuPont product information for Delrin 100 NC010; 'The data listed here fall within the normal range of product properties')1,220kg/m³sourcetypical
Strength to weight48.6kN·m/kg2.5x higher19.4kN·m/kg
Stiffness to weight1.97MN·m/kg35.9x higher0.0549MN·m/kg
Poisson's ratio0.35sourcetypicalnot sourced
Shear modulus1.04GPanot sourced
Bulk modulus3.11GPanot sourced
Speed of sound1,404m/s234m/s
Thermal
Thermal conductivity0.4W/m·Ksourcetypicalnot sourced
Thermal expansion122µm/m·Ksourcemean, 29 to 60 °Cnot sourced
100 mm part over a 50 °C swing610µm growthnot sourced
Specific heat1,465J/kg·Ksourceaverage -18 to 100 °C, Delrin acetal resins (not grade-specific)not sourced
Heats up and cools (diffusivity)0.192mm²/snot sourced
Thermal shock resistance52.5W/mnot sourced
Melting point175°Csourcecrystalline melting point217°Csourcetypical
Max service temperature125°CsourceHDT 1.8 MPa (annealed)50.3°CsourceHDT 0.455 MPa (printed specimens)
Values forDuPont Delrin 100 acetal homopolymer, Table 2 'Typical Properties of Delrin Acetal Resins' (ASTM methods), Delrin Design Guide Module III hosted on delrin.comUltimaker TPU 95A, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 29, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic TPU is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic POM/Acetal stronger than Plastic TPU?

Plastic POM/Acetal is stronger: its yield strength is 69 MPa against tensile strength 23.7 MPa for Plastic TPU (2.91x).

Which is lighter, Plastic POM/Acetal or Plastic TPU?

Plastic TPU is lighter: 1,220 kg/m³ against 1,420 kg/m³ for Plastic POM/Acetal.

Which is stiffer, Plastic POM/Acetal or Plastic TPU?

Plastic POM/Acetal is stiffer: Young's modulus 2.8 GPa against 0.067 GPa for Plastic TPU, so the same part in Plastic POM/Acetal deflects less under the same load.

Which is lighter for the same job, Plastic POM/Acetal or Plastic TPU?

For the same stiffness or strength: Plastic POM/Acetal is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic POM/AcetalPlastic TPU
Stiff rod or tie (tension)lighter35.9x heavier
Stiff beam (bending)lighter5.55x heavier
Stiff panel or platelighter2.98x heavier
Strong rod or tielighter2.5x heavier
Strong beamlighter1.75x heavier
Strong panel or platelighter47% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic POM/AcetalPlastic TPU
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic POM/AcetalPlastic TPU
Strength against density