Materials / Compare

Plastic POM/Acetal vs. SLA Resin Tough 2000

Compare Plastic POM/Acetal vs. SLA Resin Tough 2000 strength, stiffness, weight and thermal properties.

Change either side
Plastic POM/AcetalBulk polymer (molded or machined)
SLA Resin Tough 20003D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength69MPasourcetypical (single ASTM D638 tensile strength)40.4MPasourcetypical
Ultimate tensile strength69MPasourcetypical1.71x stronger40.4MPasourcetypical
Compressive strength124MPasourcecompressive stress at 10% deformationnot sourced
Flexural strength99MPasourceflexural yield strength, typical67MPasourcetypical
Elongation at break75%sourcetypical79%sourcetypical
Young's modulus (stiffness)2.8GPasourcetypical1.56x stiffer1.8GPasourcetypical
Density1,420kg/m³sourcetypical (DuPont product information for Delrin 100 NC010; 'The data listed here fall within the normal range of product properties')1,090kg/m³sourcetypical
Strength to weight48.6kN·m/kg31% higher37.1kN·m/kg
Stiffness to weight1.97MN·m/kg19% higher1.65MN·m/kg
Poisson's ratio0.35sourcetypicalnot sourced
Shear modulus1.04GPanot sourced
Bulk modulus3.11GPanot sourced
Speed of sound1,404m/s1,285m/s
Thermal
Thermal conductivity0.4W/m·Ksourcetypicalnot sourced
Thermal expansion122µm/m·Ksourcemean, 29 to 60 °C134µm/m·Ksourcemean 0-150 °C
100 mm part over a 50 °C swing610µm growth10% less671µm growth
Specific heat1,465J/kg·Ksourceaverage -18 to 100 °C, Delrin acetal resins (not grade-specific)not sourced
Heats up and cools (diffusivity)0.192mm²/snot sourced
Thermal shock resistance52.5W/mnot sourced
Melting point175°Csourcecrystalline melting pointnot sourced
Glass transitionnot sourced112°CsourceDMA
Max service temperature125°CsourceHDT 1.8 MPa (annealed)57°CsourceHDT 1.8 MPa
Values forDuPont Delrin 100 acetal homopolymer, Table 2 'Typical Properties of Delrin Acetal Resins' (ASTM methods), Delrin Design Guide Module III hosted on delrin.comFormlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic POM/Acetal stronger than SLA Resin Tough 2000?

Plastic POM/Acetal is stronger: its yield strength is 69 MPa against 40.4 MPa for SLA Resin Tough 2000 (1.71x).

Which is lighter, Plastic POM/Acetal or SLA Resin Tough 2000?

SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 1,420 kg/m³ for Plastic POM/Acetal.

Which is stiffer, Plastic POM/Acetal or SLA Resin Tough 2000?

Plastic POM/Acetal is stiffer: Young's modulus 2.8 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Plastic POM/Acetal deflects less under the same load.

Which is lighter for the same job, Plastic POM/Acetal or SLA Resin Tough 2000?

For the same stiffness or strength: Plastic POM/Acetal is lighter for a stiff rod or tie (tension), strong rod or tie, strong beam; SLA Resin Tough 2000 is lighter for a stiff beam (bending), stiff panel or plate.

Part that must bePlastic POM/AcetalSLA Resin Tough 2000
Stiff rod or tie (tension)lighter19% heavier
Stiff beam (bending)4% heavierlighter
Stiff panel or plate12% heavierlighter
Strong rod or tielighter31% heavier
Strong beamlighter10% heavier
Strong panel or plateabout equalabout equal

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which expands less with temperature?

Plastic POM/Acetal expands less: 122 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic POM/AcetalSLA Resin Tough 2000
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic POM/AcetalSLA Resin Tough 2000
Strength against density

Related comparisons