BASF Ultradur B 4300 G6 (PBT, 30% glass fibre), injection moulding grade; product information sheet 09/2026, typical values for uncoloured product at 23 °C.
DuPont Delrin 100 acetal homopolymer, Table 2 'Typical Properties of Delrin Acetal Resins' (ASTM methods), Delrin Design Guide Module III hosted on delrin.com
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Is Plastic PBT GF30 stronger than Plastic POM/Acetal?
Plastic PBT GF30 is stronger: its tensile strength is 140 MPa against yield strength 69 MPa for Plastic POM/Acetal (2.03x).
Which is lighter, Plastic PBT GF30 or Plastic POM/Acetal?
Plastic POM/Acetal is lighter: 1,420 kg/m³ against 1,530 kg/m³ for Plastic PBT GF30.
Which is stiffer, Plastic PBT GF30 or Plastic POM/Acetal?
Plastic PBT GF30 is stiffer: Young's modulus 9.8 GPa against 2.8 GPa for Plastic POM/Acetal, so the same part in Plastic PBT GF30 deflects less under the same load.
Which is lighter for the same job, Plastic PBT GF30 or Plastic POM/Acetal?
For the same stiffness or strength: Plastic PBT GF30 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Plastic PBT GF30
Plastic POM/Acetal
Stiff rod or tie (tension)
lighter
3.25x heavier
Stiff beam (bending)
lighter
1.74x heavier
Stiff panel or plate
lighter
41% heavier
Strong rod or tie
lighter
1.88x heavier
Strong beam
lighter
49% heavier
Strong panel or plate
lighter
32% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which conducts heat better, Plastic PBT GF30 or Plastic POM/Acetal?
Plastic POM/Acetal conducts heat better: 0.4 W/m·K against 0.27 W/m·K for Plastic PBT GF30.
Which expands less with temperature?
Plastic PBT GF30 expands less: 25 µm/m·K against 122 µm/m·K for Plastic POM/Acetal.