Materials / Compare

Plastic PLA vs. Plastic POM/Acetal

Compare Plastic PLA vs. Plastic POM/Acetal strength, stiffness, weight and thermal properties.

Change either side
Plastic PLA3D printed (FDM)
Plastic POM/AcetalBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength52.5MPasourcetypical69MPasourcetypical (single ASTM D638 tensile strength)
Ultimate tensile strength52.5MPasourcetypical, peak stress (= stress at yield)69MPasourcetypical
Compressive strengthnot sourced124MPasourcecompressive stress at 10% deformation
Flexural strength96.8MPasourcetypical99MPasourceflexural yield strength, typical
Elongation at break7.8%sourcetypical75%sourcetypical9.62x more ductile
Young's modulus (stiffness)3.25GPasourcetypical16% stiffer2.8GPasourcetypical
Density1,240kg/m³sourcetypical1,420kg/m³sourcetypical (DuPont product information for Delrin 100 NC010; 'The data listed here fall within the normal range of product properties')
Strength to weight42.3kN·m/kg48.6kN·m/kg15% higher
Stiffness to weight2.62MN·m/kg33% higher1.97MN·m/kg
Poisson's rationot sourced0.35sourcetypical
Shear modulusnot sourced1.04GPa
Bulk modulusnot sourced3.11GPa
Speed of sound1,619m/s1,404m/s
Thermal
Thermal conductivity0.13W/m·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C0.4W/m·Ksourcetypical
Thermal expansionnot sourced122µm/m·Ksourcemean, 29 to 60 °C
100 mm part over a 50 °C swingnot sourced610µm growth
Specific heat1,200J/kg·Ksourcebase material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C1,465J/kg·Ksourceaverage -18 to 100 °C, Delrin acetal resins (not grade-specific)
Heats up and cools (diffusivity)0.0874mm²/s0.192mm²/s2.2x faster
Thermal shock resistancenot sourced52.5W/m
Melting point152°Csourcetypical175°Csourcecrystalline melting point
Glass transition59.1°Csourcetypicalnot sourced
Max service temperature58.8°CsourceHDT 0.455 MPa (printed specimens)125°CsourceHDT 1.8 MPa (annealed)
Values forUltimaker PLA, 3D-printed specimens, XY (flat) orientation; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS dated April 20, 2022.DuPont Delrin 100 acetal homopolymer, Table 2 'Typical Properties of Delrin Acetal Resins' (ASTM methods), Delrin Design Guide Module III hosted on delrin.com

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PLA is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic PLA stronger than Plastic POM/Acetal?

Plastic POM/Acetal is stronger: its yield strength is 69 MPa against 52.5 MPa for Plastic PLA (31%).

Which is lighter, Plastic PLA or Plastic POM/Acetal?

Plastic PLA is lighter: 1,240 kg/m³ against 1,420 kg/m³ for Plastic POM/Acetal.

Which is stiffer, Plastic PLA or Plastic POM/Acetal?

Plastic PLA is stiffer: Young's modulus 3.25 GPa against 2.8 GPa for Plastic POM/Acetal, so the same part in Plastic PLA deflects less under the same load.

Which is lighter for the same job, Plastic PLA or Plastic POM/Acetal?

For the same stiffness or strength: Plastic PLA is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Plastic POM/Acetal is lighter for a strong rod or tie, strong beam.

Part that must bePlastic PLAPlastic POM/Acetal
Stiff rod or tie (tension)lighter33% heavier
Stiff beam (bending)lighter23% heavier
Stiff panel or platelighter20% heavier
Strong rod or tie15% heavierlighter
Strong beam5% heavierlighter
Strong panel or plateabout equalabout equal

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic PLA or Plastic POM/Acetal?

Plastic POM/Acetal stretches further before it breaks: 75% elongation at break against 7.8% for Plastic PLA.

Which conducts heat better, Plastic PLA or Plastic POM/Acetal?

Plastic POM/Acetal conducts heat better: 0.4 W/m·K against 0.13 W/m·K for Plastic PLA.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PLAPlastic POM/Acetal
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PLAPlastic POM/Acetal
Strength against density