Materials / Compare

Plastic ABS vs. Plastic POM/Acetal

Compare Plastic ABS vs. Plastic POM/Acetal strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS3D printed (FDM)
Plastic POM/AcetalBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength38.1MPasourcetypical69MPasourcetypical (single ASTM D638 tensile strength)
Ultimate tensile strength38.1MPasourcetypical, peak stress (= stress at yield)69MPasourcetypical
Compressive strengthnot sourced124MPasourcecompressive stress at 10% deformation
Flexural strength61.1MPasourcetypical99MPasourceflexural yield strength, typical
Elongation at break4.6%sourcetypical75%sourcetypical16.3x more ductile
Young's modulus (stiffness)1.96GPasourcetypical2.8GPasourcetypical43% stiffer
Density1,100kg/m³sourcetypical1,420kg/m³sourcetypical (DuPont product information for Delrin 100 NC010; 'The data listed here fall within the normal range of product properties')
Strength to weight34.6kN·m/kg48.6kN·m/kg40% higher
Stiffness to weight1.78MN·m/kg1.97MN·m/kg11% higher
Poisson's ratio0.39sourcebase material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)0.35sourcetypical
Shear modulus0.706GPa1.04GPa47% stiffer in shear
Bulk modulus2.97GPa3.11GPa
Speed of sound1,336m/s1,404m/s
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typical0.4W/m·Ksourcetypical
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, range122µm/m·Ksourcemean, 29 to 60 °C
100 mm part over a 50 °C swing475µm growth28% less610µm growth
Specific heatnot sourced1,465J/kg·Ksourceaverage -18 to 100 °C, Delrin acetal resins (not grade-specific)
Heats up and cools (diffusivity)not sourced0.192mm²/s
Thermal shock resistance21.2W/m52.5W/m2.48x more resistant
Melting pointnot sourced175°Csourcecrystalline melting point
Glass transition101°Csourcetypicalnot sourced
Max service temperature86.6°CsourceHDT 0.455 MPa (printed specimens)125°CsourceHDT 1.8 MPa (annealed)
Values forUltimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.DuPont Delrin 100 acetal homopolymer, Table 2 'Typical Properties of Delrin Acetal Resins' (ASTM methods), Delrin Design Guide Module III hosted on delrin.com

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic ABS is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS stronger than Plastic POM/Acetal?

Plastic POM/Acetal is stronger: its yield strength is 69 MPa against 38.1 MPa for Plastic ABS (1.81x).

Which is lighter, Plastic ABS or Plastic POM/Acetal?

Plastic ABS is lighter: 1,100 kg/m³ against 1,420 kg/m³ for Plastic POM/Acetal.

Which is stiffer, Plastic ABS or Plastic POM/Acetal?

Plastic POM/Acetal is stiffer: Young's modulus 2.8 GPa against 1.96 GPa for Plastic ABS, so the same part in Plastic POM/Acetal deflects less under the same load.

Which is lighter for the same job, Plastic ABS or Plastic POM/Acetal?

For the same stiffness or strength: Plastic ABS is lighter for a stiff beam (bending), stiff panel or plate; Plastic POM/Acetal is lighter for a stiff rod or tie (tension), strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABSPlastic POM/Acetal
Stiff rod or tie (tension)11% heavierlighter
Stiff beam (bending)lighter8% heavier
Stiff panel or platelighter15% heavier
Strong rod or tie40% heavierlighter
Strong beam15% heavierlighter
Strong panel or plate4% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic ABS or Plastic POM/Acetal?

Plastic POM/Acetal stretches further before it breaks: 75% elongation at break against 4.6% for Plastic ABS.

Which conducts heat better, Plastic ABS or Plastic POM/Acetal?

Plastic POM/Acetal conducts heat better: 0.4 W/m·K against 0.17 W/m·K for Plastic ABS.

Which expands less with temperature?

Plastic ABS expands less: 95 µm/m·K against 122 µm/m·K for Plastic POM/Acetal.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABSPlastic POM/Acetal
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABSPlastic POM/Acetal
Strength against density