Materials / Compare

Plastic ABS vs. Plastic PETG

Compare Plastic ABS vs. Plastic PETG strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS3D printed (FDM)
Plastic PETG3D printed (FDM)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength38.1MPasourcetypical46.2MPasourcetypical21% stronger
Ultimate tensile strength38.1MPasourcetypical, peak stress (= stress at yield)46.2MPasourcetypical, peak stress (= stress at yield)21% stronger
Flexural strength61.1MPasourcetypical78.9MPasourcetypical29% stronger in bending
Elongation at break4.6%sourcetypical7.6%sourcetypical1.65x more ductile
Young's modulus (stiffness)1.96GPasourcetypical1.94GPasourcetypical
Density1,100kg/m³sourcetypical15% lighter1,270kg/m³sourcetypical
Strength to weight34.6kN·m/kg36.4kN·m/kg5% higher
Stiffness to weight1.78MN·m/kg17% higher1.53MN·m/kg
Poisson's ratio0.39sourcebase material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)not sourced
Shear modulus0.706GPanot sourced
Bulk modulus2.97GPanot sourced
Speed of sound1,336m/s1,236m/s
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typical0.21W/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, range51µm/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical
100 mm part over a 50 °C swing475µm growth255µm growth1.86x less
Specific heatnot sourced1,300J/kg·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)
Heats up and cools (diffusivity)not sourced0.127mm²/s
Thermal shock resistance21.2W/mnot sourced
Glass transition101°Csourcetypical77.4°Csourcetypical
Max service temperature86.6°CsourceHDT 0.455 MPa (printed specimens)14% hotter76.2°CsourceHDT 0.455 MPa (printed specimens)
Values forUltimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.Ultimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic ABS and Plastic PETG are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS stronger than Plastic PETG?

Plastic PETG is stronger: its yield strength is 46.2 MPa against 38.1 MPa for Plastic ABS (21%).

Which is lighter, Plastic ABS or Plastic PETG?

Plastic ABS is lighter: 1,100 kg/m³ against 1,270 kg/m³ for Plastic PETG.

Which is stiffer, Plastic ABS or Plastic PETG?

Plastic ABS is stiffer: Young's modulus 1.96 GPa against 1.94 GPa for Plastic PETG, so the same part in Plastic ABS deflects less under the same load.

Which is lighter for the same job, Plastic ABS or Plastic PETG?

For the same stiffness or strength: Plastic ABS is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong beam, strong panel or plate; Plastic PETG is lighter for a strong rod or tie.

Part that must bePlastic ABSPlastic PETG
Stiff rod or tie (tension)lighter17% heavier
Stiff beam (bending)lighter16% heavier
Stiff panel or platelighter16% heavier
Strong rod or tie5% heavierlighter
Strong beamlighter2% heavier
Strong panel or platelighter5% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic ABS or Plastic PETG?

Plastic PETG stretches further before it breaks: 7.6% elongation at break against 4.6% for Plastic ABS.

Which handles higher temperatures, Plastic ABS or Plastic PETG?

Plastic ABS does: 86.6 °C against 76.2 °C for Plastic PETG, both HDT 0.455 MPa (printed specimens).

Which conducts heat better, Plastic ABS or Plastic PETG?

Plastic PETG conducts heat better: 0.21 W/m·K against 0.17 W/m·K for Plastic ABS.

Which expands less with temperature?

Plastic PETG expands less: 51 µm/m·K against 95 µm/m·K for Plastic ABS.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABSPlastic PETG
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic ABSPlastic PETG
Strength against density

Related comparisons