Materials / Compare

Plastic ABS vs. SLS PA12 Nylon

Compare Plastic ABS vs. SLS PA12 Nylon strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS3D printed (FDM)
SLS PA12 Nylon3D printed (SLS)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength38.1MPasourcetypicalnot given (tensile used)
Ultimate tensile strength38.1MPasourcetypical, peak stress (= stress at yield)48MPasourcetypical
Flexural strength61.1MPasourcetypicalnot sourced
Elongation at break4.6%sourcetypical18%sourcetypical3.91x more ductile
Young's modulus (stiffness)1.96GPasourcetypical19% stiffer1.65GPasourcetypical
Density1,100kg/m³sourcetypical930kg/m³sourcetypical18% lighter
Strength to weight34.6kN·m/kg51.6kN·m/kg49% higher
Stiffness to weight1.78MN·m/kg1.77MN·m/kg
Poisson's ratio0.39sourcebase material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)not sourced
Shear modulus0.706GPanot sourced
Bulk modulus2.97GPanot sourced
Speed of sound1,336m/s1,332m/s
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typicalnot sourced
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, rangenot sourced
100 mm part over a 50 °C swing475µm growthnot sourced
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistance21.2W/mnot sourced
Melting pointnot sourced176°Csourcetypical
Glass transition101°Csourcetypicalnot sourced
Max service temperature86.6°CsourceHDT 0.455 MPa (printed specimens)64°CsourceHDT 1.8 MPa, X orientation
Values forUltimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.EOS PA 2200 (PA12) Material Data Sheet, process parameter 'Balance' at 120 µm layer thickness, X orientation, dry (conditioned values not given). Live MDS status 04.10.2026, last changed 10.09.2026; PDF via ?topdf=... link on the same page.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic ABS and SLS PA12 Nylon are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS stronger than SLS PA12 Nylon?

SLS PA12 Nylon is stronger: its tensile strength is 48 MPa against yield strength 38.1 MPa for Plastic ABS (26%).

Which is lighter, Plastic ABS or SLS PA12 Nylon?

SLS PA12 Nylon is lighter: 930 kg/m³ against 1,100 kg/m³ for Plastic ABS.

Which is stiffer, Plastic ABS or SLS PA12 Nylon?

Plastic ABS is stiffer: Young's modulus 1.96 GPa against 1.65 GPa for SLS PA12 Nylon, so the same part in Plastic ABS deflects less under the same load.

Which is lighter for the same job, Plastic ABS or SLS PA12 Nylon?

For the same stiffness or strength: SLS PA12 Nylon is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABSSLS PA12 Nylon
Stiff rod or tie (tension)about equalabout equal
Stiff beam (bending)8% heavierlighter
Stiff panel or plate12% heavierlighter
Strong rod or tie49% heavierlighter
Strong beam38% heavierlighter
Strong panel or plate33% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic ABS or SLS PA12 Nylon?

SLS PA12 Nylon stretches further before it breaks: 18% elongation at break against 4.6% for Plastic ABS.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000DMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABSSLS PA12 Nylon
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ADMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABSSLS PA12 Nylon
Strength against density

Related comparisons