Materials / Compare

Plastic ABS (bulk/injection) vs. SLS PA12 Nylon

Compare Plastic ABS (bulk/injection) vs. SLS PA12 Nylon strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS (bulk/injection)Bulk polymer (molded or machined)
SLS PA12 Nylon3D printed (SLS)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength45MPasourcetypical, tensile stress at yield 23 °Cnot given (tensile used)
Ultimate tensile strengthnot sourced48MPasourcetypical
Flexural strength65MPasourcetypical, 23 °Cnot sourced
Elongation at break10%sourcenominal strain at break, 23 °C18%sourcetypical
Young's modulus (stiffness)2.3GPasourcetypical39% stiffer1.65GPasourcetypical
Density1,040kg/m³sourcetypical930kg/m³sourcetypical12% lighter
Strength to weight43.3kN·m/kg51.6kN·m/kg19% higher
Stiffness to weight2.21MN·m/kg25% higher1.77MN·m/kg
Poisson's ratio0.39sourcetypical, ABS family (Covestro Part and Mold Design guide, Table 3-1)not sourced
Shear modulus0.827GPanot sourced
Bulk modulus3.48GPanot sourced
Speed of sound1,487m/s1,332m/s
Thermal
Thermal conductivity0.17W/m·Ksourcetypicalnot sourced
Thermal expansion80–110µm/m·Ksourcerangenot sourced
100 mm part over a 50 °C swing475µm growthnot sourced
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistance21.4W/mnot sourced
Melting pointnot sourced176°Csourcetypical
Max service temperature94°CsourceHDT 1.8 MPa (annealed 4 h/80 °C)64°CsourceHDT 1.8 MPa, X orientation
Values forINEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)EOS PA 2200 (PA12) Material Data Sheet, process parameter 'Balance' at 120 µm layer thickness, X orientation, dry (conditioned values not given). Live MDS status 04.10.2026, last changed 10.09.2026; PDF via ?topdf=... link on the same page.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLS PA12 Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS (bulk/injection) stronger than SLS PA12 Nylon?

SLS PA12 Nylon is stronger: its tensile strength is 48 MPa against yield strength 45 MPa for Plastic ABS (bulk/injection) (7%).

Which is lighter, Plastic ABS (bulk/injection) or SLS PA12 Nylon?

SLS PA12 Nylon is lighter: 930 kg/m³ against 1,040 kg/m³ for Plastic ABS (bulk/injection).

Which is stiffer, Plastic ABS (bulk/injection) or SLS PA12 Nylon?

Plastic ABS (bulk/injection) is stiffer: Young's modulus 2.3 GPa against 1.65 GPa for SLS PA12 Nylon, so the same part in Plastic ABS (bulk/injection) deflects less under the same load.

Which is lighter for the same job, Plastic ABS (bulk/injection) or SLS PA12 Nylon?

For the same stiffness or strength: Plastic ABS (bulk/injection) is lighter for a stiff rod or tie (tension), stiff beam (bending); SLS PA12 Nylon is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABS (bulk/injection)SLS PA12 Nylon
Stiff rod or tie (tension)lighter25% heavier
Stiff beam (bending)lighter6% heavier
Stiff panel or plateabout equalabout equal
Strong rod or tie19% heavierlighter
Strong beam17% heavierlighter
Strong panel or plate15% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000DMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABS (bulk/injection)SLS PA12 Nylon
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ADMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABS (bulk/injection)SLS PA12 Nylon
Strength against density

Related comparisons