Materials / Compare

Plastic Polypropylene vs. Plastic PTFE

Compare Plastic Polypropylene vs. Plastic PTFE strength, stiffness, weight and thermal properties.

Change either side
Plastic PolypropyleneBulk polymer (molded or machined)
Plastic PTFEBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength33MPasourcetypical, tensile stress at yield ISO 5279MPasourcetypical yield strength at 23 °C (Teflon PTFE, Table 8)
Ultimate tensile strengthnot sourced39.3MPasourcetypical, skived tape 0.13 mm
Elongation at breaknot sourced350%sourcetypical, skived tape 0.13 mm
Young's modulus (stiffness)1.45GPasourcetypical, tensile modulus ISO 527not sourced
Density900kg/m³sourcetypical, 23 °C ISO 1183-12,160kg/m³sourcetypical (standard specific gravity, ASTM D4894)
Strength to weight36.7kN·m/kg8.8x higher4.17kN·m/kg
Stiffness to weight1.61MN·m/kgnot sourced
Poisson's ratio0.42sourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)0.46sourcetypical, 23 °C (Teflon PTFE resins, Chemours handbook)
Shear modulus0.511GPanot sourced
Bulk modulus3.02GPanot sourced
Speed of sound1,269m/snot sourced
Thermal
Thermal conductivity0.17–0.22W/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)0.25W/m·Ksourcetypical, granular resin, 4.6 mm specimen
Thermal expansion80–100µm/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)100µm/m·Ksourcetypical, granular resin, 23-60 °C (ASTM E228)
100 mm part over a 50 °C swing450µm growth11% less500µm growth
Specific heatnot sourced1,400J/kg·Ksourcetypical, granular resin, 20 °C (ASTM D4591)
Heats up and cools (diffusivity)not sourced0.0827mm²/s
Thermal shock resistance28.6W/mnot sourced
Melting pointnot sourced327°Csourcesecond melting peak (sintered polymer), +/-10
Max service temperature90°CsourceHDT 0.45 MPa (ISO 75B), unannealed260°Csourceservice temperature (Chemours general Teflon PTFE statement)
Values forLyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO valuesChemours Teflon PTFE 7C X granular molding resin, typical values (tensile/elongation measured on 0.13 mm skived tape)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic Polypropylene stronger than Plastic PTFE?

Plastic Polypropylene is stronger: its yield strength is 33 MPa against 9 MPa for Plastic PTFE (3.67x).

Which is lighter, Plastic Polypropylene or Plastic PTFE?

Plastic Polypropylene is lighter: 900 kg/m³ against 2,160 kg/m³ for Plastic PTFE.

Which is lighter for the same job, Plastic Polypropylene or Plastic PTFE?

For the same stiffness or strength: Plastic Polypropylene is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PolypropylenePlastic PTFE
Strong rod or tielighter8.8x heavier
Strong beamlighter5.71x heavier
Strong panel or platelighter4.6x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Polypropylene or Plastic PTFE?

Plastic PTFE conducts heat better: 0.25 W/m·K against 0.195 W/m·K for Plastic Polypropylene.

Which expands less with temperature?

Plastic Polypropylene expands less: 90 µm/m·K against 100 µm/m·K for Plastic PTFE.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Polypropylene
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PolypropylenePlastic PTFE
Strength against density

Related comparisons