Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength5.1MPasourcemodulus of rupture (no direct tensile value)18.4MPasourcetypical
Compressive strength77.9MPasourcemean unit compressive strength, solid extruded brick (survey mean; SD 30.8 MPa)not sourced
Flexural strengthnot sourced31.8MPasourcetypical
Elongation at breaknot sourced1.4%sourcetypical
Young's modulus (stiffness)not sourced1.59GPasourcetypical
Density2,082kg/m³sourceface brick density row used for k (BIA notes most fired clay brick 120-130 lb/ft3)1,023kg/m³sourcetypical
Strength to weight2.45kN·m/kg18kN·m/kg7.34x higher
Stiffness to weightnot sourced1.55MN·m/kg
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of soundnot sourced1,246m/s
Thermal
Thermal conductivity0.92–1.12W/m·Ksourcerange for 130 lb/ft3 face brick (ASHRAE 2013 via BIA)0.17W/m·Ksourcebase material: INEOS Styrolution PS 486N injection-molding HIPS, typical
Thermal expansion7.2µm/m·KsourceTMS Code average coefficient, clay/shale unit masonry80µm/m·Ksourcebase material: INEOS Styrolution PS 486N injection-molding HIPS, typical
100 mm part over a 50 °C swing36µm growth11.1x less400µm growth
Specific heat837J/kg·Ksourcevalue used in BIA heat-capacity sample calculationnot sourced
Heats up and cools (diffusivity)0.585mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Glass transitionnot sourced99°Csourcetypical
Max service temperaturenot sourced86°CsourceHDT 1.8 MPa
Values forSolid extruded clay/shale brick units (BIA 1993 manufacturer survey, TN 3A 2024); face brick of 130 lb/ft3 for thermal properties (BIA TN 4, from ASHRAE 2013); CTE is the TMS Code value for clay/shale masonryBASF Forward AM (BASF 3D Printing Solutions) Ultrafuse HiPS, TDS v2.2 (13.11.2019), printed specimens, XY 'Flat'. Specimen print settings are not stated; recommended processing on the sheet: nozzle 240-260 °C, bed 100-120 °C, 40-80 mm/s. Product is discontinued (Forward AM product page) but the TDS is still served by Forward AM.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM HIPS is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Brick stronger than FDM HIPS?

FDM HIPS is stronger: its tensile strength is 18.4 MPa against 5.1 MPa for Brick (3.61x).

Which is lighter, Brick or FDM HIPS?

FDM HIPS is lighter: 1,023 kg/m³ against 2,082 kg/m³ for Brick.

Which is lighter for the same job, Brick or FDM HIPS?

For the same stiffness or strength: FDM HIPS is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beBrickFDM HIPS
Strong rod or tie7.34x heavierlighter
Strong beam4.79x heavierlighter
Strong panel or plate3.87x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Brick or FDM HIPS?

Brick conducts heat better: 1.02 W/m·K against 0.17 W/m·K for FDM HIPS.

Which expands less with temperature?

Brick expands less: 7.2 µm/m·K against 80 µm/m·K for FDM HIPS.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelFDM HIPS
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickFDM HIPS
Strength against density

Related comparisons