Materials / FDM
FDM HIPSFDM HIPS strength, stiffness, density and thermal properties, with their source.
A bracket in FDM HIPS, 3D-printed (layer lines) finish.
Process 3D printed (FDM) Mechanical Yield strength not given (tensile used) Ultimate tensile strength 18.4 MPa source typical Flexural strength 31.8 MPa source typical Elongation at break 1.4 % source typical Young's modulus (stiffness) 1.59 GPa source typical Density 1,023 kg/m³ source typical Strength to weight 18 kN·m/kg Stiffness to weight 1.55 MN·m/kg Poisson's ratio not sourced Shear modulus not sourced Bulk modulus not sourced Speed of sound 1,246 m/s Thermal Thermal conductivity 0.17 W/m·K source base material: INEOS Styrolution PS 486N injection-molding HIPS, typical Thermal expansion 80 µm/m·K source base material: INEOS Styrolution PS 486N injection-molding HIPS, typical 100 mm part over a 50 °C swing 400 µm growth Specific heat not sourced Heats up and cools (diffusivity) not sourced Thermal shock resistance not sourced Glass transition 99 °C source typical Max service temperature 86 °C source HDT 1.8 MPa Values for BASF Forward AM (BASF 3D Printing Solutions) Ultrafuse HiPS, TDS v2.2 (13.11.2019), printed specimens, XY 'Flat'. Specimen print settings are not stated; recommended processing on the sheet: nozzle 240-260 °C, bed 100-120 °C, 40-80 mm/s. Product is discontinued (Forward AM product page) but the TDS is still served by Forward AM.
FDM HIPS is 3D printed: its properties depend on build direction and print settings; these are typical values.
Among 59 materials 1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel FDM HIPS Stiffness against density 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Rubber Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick FDM HIPS Strength against density