Materials / Compare

FDM HIPS vs. SLA Resin Tough 2000

Compare FDM HIPS vs. SLA Resin Tough 2000 strength, stiffness, weight and thermal properties.

Change either side
FDM HIPS3D printed (FDM)
SLA Resin Tough 20003D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)40.4MPasourcetypical
Ultimate tensile strength18.4MPasourcetypical40.4MPasourcetypical2.2x stronger
Flexural strength31.8MPasourcetypical67MPasourcetypical2.11x stronger in bending
Elongation at break1.4%sourcetypical79%sourcetypical56.4x more ductile
Young's modulus (stiffness)1.59GPasourcetypical1.8GPasourcetypical13% stiffer
Density1,023kg/m³sourcetypical1,090kg/m³sourcetypical
Strength to weight18kN·m/kg37.1kN·m/kg2.06x higher
Stiffness to weight1.55MN·m/kg1.65MN·m/kg6% higher
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,246m/s1,285m/s
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution PS 486N injection-molding HIPS, typicalnot sourced
Thermal expansion80µm/m·Ksourcebase material: INEOS Styrolution PS 486N injection-molding HIPS, typical134µm/m·Ksourcemean 0-150 °C
100 mm part over a 50 °C swing400µm growth1.68x less671µm growth
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistancenot sourcednot sourced
Glass transition99°Csourcetypical112°CsourceDMA
Max service temperature86°CsourceHDT 1.8 MPa1.51x hotter57°CsourceHDT 1.8 MPa
Values forBASF Forward AM (BASF 3D Printing Solutions) Ultrafuse HiPS, TDS v2.2 (13.11.2019), printed specimens, XY 'Flat'. Specimen print settings are not stated; recommended processing on the sheet: nozzle 240-260 °C, bed 100-120 °C, 40-80 mm/s. Product is discontinued (Forward AM product page) but the TDS is still served by Forward AM.Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM HIPS and SLA Resin Tough 2000 are 3D printed: their properties depend on build direction and print settings; these are typical values.

Questions

Is FDM HIPS stronger than SLA Resin Tough 2000?

SLA Resin Tough 2000 is stronger: its yield strength is 40.4 MPa against tensile strength 18.4 MPa for FDM HIPS (2.2x).

Which is lighter, FDM HIPS or SLA Resin Tough 2000?

FDM HIPS is lighter: 1,023 kg/m³ against 1,090 kg/m³ for SLA Resin Tough 2000.

Which is stiffer, FDM HIPS or SLA Resin Tough 2000?

SLA Resin Tough 2000 is stiffer: Young's modulus 1.8 GPa against 1.59 GPa for FDM HIPS, so the same part in SLA Resin Tough 2000 deflects less under the same load.

Which is lighter for the same job, FDM HIPS or SLA Resin Tough 2000?

For the same stiffness or strength: FDM HIPS is lighter for a stiff panel or plate; SLA Resin Tough 2000 is lighter for a stiff rod or tie (tension), strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM HIPSSLA Resin Tough 2000
Stiff rod or tie (tension)6% heavierlighter
Stiff beam (bending)about equalabout equal
Stiff panel or platelighter2% heavier
Strong rod or tie2.06x heavierlighter
Strong beam1.59x heavierlighter
Strong panel or plate39% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, FDM HIPS or SLA Resin Tough 2000?

SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 1.4% for FDM HIPS.

Which handles higher temperatures, FDM HIPS or SLA Resin Tough 2000?

FDM HIPS does: 86 °C against 57 °C for SLA Resin Tough 2000, both HDT 1.8 MPa.

Which expands less with temperature?

FDM HIPS expands less: 80 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFSLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelFDM HIPSSLA Resin Tough 2000
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFSLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickFDM HIPSSLA Resin Tough 2000
Strength against density

Related comparisons