Materials / Compare

FDM HIPS vs. Rubber

Compare FDM HIPS vs. Rubber strength, stiffness, weight and thermal properties.

Change either side
FDM HIPS3D printed (FDM)
RubberBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strength18.4MPasourcetypical23MPasourcetypical25% stronger
Flexural strength31.8MPasourcetypicalnot sourced
Elongation at break1.4%sourcetypical830%sourcetypical593x more ductile
Young's modulus (stiffness)1.59GPasourcetypicalnot sourced
Density1,023kg/m³sourcetypical960kg/m³sourcetypical (specific gravity)
Strength to weight18kN·m/kg24kN·m/kg33% higher
Stiffness to weight1.55MN·m/kgnot sourced
Poisson's rationot sourced0.5sourcegovernment (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,246m/snot sourced
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution PS 486N injection-molding HIPS, typical0.151W/m·Ksourcegovernment selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C
Thermal expansion80µm/m·Ksourcebase material: INEOS Styrolution PS 486N injection-molding HIPS, typicalnot sourced
100 mm part over a 50 °C swing400µm growthnot sourced
Specific heatnot sourced1,881J/kg·Ksourcegovernment (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C
Heats up and cools (diffusivity)not sourced0.0836mm²/s
Thermal shock resistancenot sourcednot sourced
Glass transition99°Csourcetypicalnot sourced
Max service temperature86°CsourceHDT 1.8 MPa70°Csourcecontinuous use operating range
Values forBASF Forward AM (BASF 3D Printing Solutions) Ultrafuse HiPS, TDS v2.2 (13.11.2019), printed specimens, XY 'Flat'. Specimen print settings are not stated; recommended processing on the sheet: nozzle 240-260 °C, bed 100-120 °C, 40-80 mm/s. Product is discontinued (Forward AM product page) but the TDS is still served by Forward AM.Weir Minerals Linatex Premium rubber (95 % natural rubber), typical physical properties, spec sheet WMD0118/202305

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM HIPS is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is FDM HIPS stronger than Rubber?

Rubber is stronger: its tensile strength is 23 MPa against 18.4 MPa for FDM HIPS (25%).

Which is lighter, FDM HIPS or Rubber?

Rubber is lighter: 960 kg/m³ against 1,023 kg/m³ for FDM HIPS.

Which is lighter for the same job, FDM HIPS or Rubber?

For the same stiffness or strength: Rubber is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM HIPSRubber
Strong rod or tie33% heavierlighter
Strong beam24% heavierlighter
Strong panel or plate19% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, FDM HIPS or Rubber?

Rubber stretches further before it breaks: 830% elongation at break against 1.4% for FDM HIPS.

Which conducts heat better, FDM HIPS or Rubber?

FDM HIPS conducts heat better: 0.17 W/m·K against 0.151 W/m·K for Rubber.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelFDM HIPS
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickFDM HIPSRubber
Strength against density

Related comparisons