Mechanical
Yield strength24MPasourcetypical, tensile stress at yield 23 °C, 50 mm/min ISO 527not given (tensile used)
Ultimate tensile strengthnot sourced23MPasourcetypical
Elongation at breaknot sourced830%sourcetypical
Young's modulus (stiffness)0.9GPasourcetypical, tensile modulus 23 °C ISO 527not sourced
Density950kg/m³sourcetypical, ISO 1183960kg/m³sourcetypical (specific gravity)
Strength to weight25.3kN·m/kg5% higher24kN·m/kg
Stiffness to weight0.947MN·m/kgnot sourced
Poisson's ratio0.4–0.45sourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)0.5sourcegovernment (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).
Shear modulus0.316GPanot sourced
Bulk modulus2GPanot sourced
Speed of sound973m/snot sourced
Thermal
Thermal conductivity0.4–0.49W/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)0.151W/m·Ksourcegovernment selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C
Thermal expansion120µm/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)not sourced
100 mm part over a 50 °C swing600µm growthnot sourced
Specific heat2,250J/kg·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)1,881J/kg·Ksourcegovernment (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C
Heats up and cools (diffusivity)0.208mm²/s2.49x faster0.0836mm²/s
Thermal shock resistance56.9W/mnot sourced
Max service temperaturenot sourced70°Csourcecontinuous use operating range
Values forLyondellBasell Hostalen 23050 B high density polyethylene, typical ISO valuesWeir Minerals Linatex Premium rubber (95 % natural rubber), typical physical properties, spec sheet WMD0118/202305

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic HDPE stronger than Rubber?

Plastic HDPE is stronger: its yield strength is 24 MPa against tensile strength 23 MPa for Rubber (4%).

Which is lighter, Plastic HDPE or Rubber?

Plastic HDPE is lighter: 950 kg/m³ against 960 kg/m³ for Rubber.

Which is lighter for the same job, Plastic HDPE or Rubber?

For the same stiffness or strength: Plastic HDPE is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic HDPERubber
Strong rod or tielighter5% heavier
Strong beamlighter4% heavier
Strong panel or platelighter3% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic HDPE or Rubber?

Plastic HDPE conducts heat better: 0.445 W/m·K against 0.151 W/m·K for Rubber.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic HDPE
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic HDPERubber
Strength against density

Related comparisons