Materials / Compare

Plastic HDPE vs. SLA Resin Tough 2000

Compare Plastic HDPE vs. SLA Resin Tough 2000 strength, stiffness, weight and thermal properties.

Change either side
Plastic HDPEBulk polymer (molded or machined)
SLA Resin Tough 20003D printed (SLA resin)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength24MPasourcetypical, tensile stress at yield 23 °C, 50 mm/min ISO 52740.4MPasourcetypical
Ultimate tensile strengthnot sourced40.4MPasourcetypical
Flexural strengthnot sourced67MPasourcetypical
Elongation at breaknot sourced79%sourcetypical
Young's modulus (stiffness)0.9GPasourcetypical, tensile modulus 23 °C ISO 5271.8GPasourcetypical
Density950kg/m³sourcetypical, ISO 11831,090kg/m³sourcetypical
Strength to weight25.3kN·m/kg37.1kN·m/kg47% higher
Stiffness to weight0.947MN·m/kg1.65MN·m/kg1.74x higher
Poisson's ratio0.4–0.45sourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)not sourced
Shear modulus0.316GPanot sourced
Bulk modulus2GPanot sourced
Speed of sound973m/s1,285m/s
Thermal
Thermal conductivity0.4–0.49W/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)not sourced
Thermal expansion120µm/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)134µm/m·Ksourcemean 0-150 °C
100 mm part over a 50 °C swing600µm growth12% less671µm growth
Specific heat2,250J/kg·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)not sourced
Heats up and cools (diffusivity)0.208mm²/snot sourced
Thermal shock resistance56.9W/mnot sourced
Glass transitionnot sourced112°CsourceDMA
Max service temperaturenot sourced57°CsourceHDT 1.8 MPa
Values forLyondellBasell Hostalen 23050 B high density polyethylene, typical ISO valuesFormlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic HDPE stronger than SLA Resin Tough 2000?

SLA Resin Tough 2000 is stronger: its yield strength is 40.4 MPa against 24 MPa for Plastic HDPE (1.68x).

Which is lighter, Plastic HDPE or SLA Resin Tough 2000?

Plastic HDPE is lighter: 950 kg/m³ against 1,090 kg/m³ for SLA Resin Tough 2000.

Which is stiffer, Plastic HDPE or SLA Resin Tough 2000?

SLA Resin Tough 2000 is stiffer: Young's modulus 1.8 GPa against 0.9 GPa for Plastic HDPE, so the same part in SLA Resin Tough 2000 deflects less under the same load.

Which is lighter for the same job, Plastic HDPE or SLA Resin Tough 2000?

For the same stiffness or strength: SLA Resin Tough 2000 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic HDPESLA Resin Tough 2000
Stiff rod or tie (tension)1.74x heavierlighter
Stiff beam (bending)23% heavierlighter
Stiff panel or plate10% heavierlighter
Strong rod or tie47% heavierlighter
Strong beam23% heavierlighter
Strong panel or plate13% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which expands less with temperature?

Plastic HDPE expands less: 120 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic HDPESLA Resin Tough 2000
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic HDPESLA Resin Tough 2000
Strength against density