Materials / Compare

Plastic ABS (bulk/injection) vs. Steel

Compare Plastic ABS (bulk/injection) vs. Steel strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS (bulk/injection)Bulk polymer (molded or machined)
SteelWrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength45MPasourcetypical, tensile stress at yield 23 °C385MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey), as reported by AISC
Ultimate tensile strengthnot sourced505MPasourcetypical: mean of 20,295 A992 flange mill-test coupons (1998 SSPC survey)
Flexural strength65MPasourcetypical, 23 °Cnot sourced
Elongation at break10%sourcenominal strain at break, 23 °Cnot sourced
Young's modulus (stiffness)2.3GPasourcetypical200GPasourcedesign value (AISC 360-16)
Density1,040kg/m³sourcetypical7,850kg/m³sourcenominal (constructional data)
Strength to weight43.3kN·m/kg49kN·m/kg13% higher
Stiffness to weight2.21MN·m/kg25.5MN·m/kg11.5x higher
Poisson's ratio0.39sourcetypical, ABS family (Covestro Part and Mold Design guide, Table 3-1)0.3sourcedesign value (AISC 360-16 Commentary)
Shear modulus0.827GPa76.9GPa93x stiffer in shear
Bulk modulus3.48GPa167GPa
Speed of sound1,487m/s5,048m/s
Thermal
Thermal conductivity0.17W/m·Ksourcetypical48W/m·Ksourcenominal at 20 °C
Thermal expansion80–110µm/m·Ksourcerange12µm/m·Ksourcenominal (constructional data, no temperature range stated)
100 mm part over a 50 °C swing475µm growth60µm growth7.92x less
Specific heatnot sourced460–480J/kg·Ksourcebase material: EN S275JR unalloyed structural steel (the EN counterpart of A36), typical, 50/100 °C
Heats up and cools (diffusivity)not sourced13mm²/s
Thermal shock resistance21.4W/m5,390W/m252x more resistant
Max service temperature94°CsourceHDT 1.8 MPa (annealed 4 h/80 °C)not sourced
Values forINEOS Styrolution Terluran GP-22 general-purpose injection-molding ABS, ISO typical values (TDS revision 08/01/2022)Generic structural steel, cited as ASTM A992 (the current US structural grade): ASTM A992 W-shapes; Fy/Fu specified minimums from AISC publications (AISC 360-16 Commentary; Modern Steel Construction); elastic constants AISC 360; physical constants from the bauforumstahl structural-steel EPD, which names A992 among covered product standards.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic ABS (bulk/injection) stronger than Steel?

Steel is stronger: its yield strength is 385 MPa against 45 MPa for Plastic ABS (bulk/injection) (8.56x).

Which is lighter, Plastic ABS (bulk/injection) or Steel?

Plastic ABS (bulk/injection) is lighter: 1,040 kg/m³ against 7,850 kg/m³ for Steel.

Which is stiffer, Plastic ABS (bulk/injection) or Steel?

Steel is stiffer: Young's modulus 200 GPa against 2.3 GPa for Plastic ABS (bulk/injection), so the same part in Steel deflects less under the same load.

Which is lighter for the same job, Plastic ABS (bulk/injection) or Steel?

For the same stiffness or strength: Plastic ABS (bulk/injection) is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.

Part that must bePlastic ABS (bulk/injection)Steel
Stiff rod or tie (tension)11.5x heavierlighter
Stiff beam (bending)24% heavierlighter
Stiff panel or platelighter1.7x heavier
Strong rod or tie13% heavierlighter
Strong beamlighter1.8x heavier
Strong panel or platelighter2.58x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic ABS (bulk/injection) or Steel?

Steel conducts heat better: 48 W/m·K against 0.17 W/m·K for Plastic ABS (bulk/injection).

Which expands less with temperature?

Steel expands less: 12 µm/m·K against 95 µm/m·K for Plastic ABS (bulk/injection).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABS (bulk/injection)Steel
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABS (bulk/injection)Steel
Strength against density

Related comparisons