Aluminum 2024-T351 vs. Rubber Compare Aluminum 2024-T351 vs. Rubber strength, stiffness, weight and thermal properties.
Change either side
Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless 304 Stainless 316 Stainless 303 Stainless 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall Aluminum 2024-T351 Wrought Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless 304 Stainless 316 Stainless 303 Stainless 17-4PH Brass C360 Brass C260 Copper C110 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall Rubber Bulk polymer (molded or machined) Try it on a partA bracket to run stress or thermal on, free in your browser Open in LessCAD Open in LessCAD Mechanical Yield strength 324 MPa source typical, 0.2% offset, .500 in dia specimen not given (tensile used) Ultimate tensile strength 469 MPa source typical 20.4x stronger 23 MPa source typical Elongation at break 19 % source typical, in 4D 830 % source typical Young's modulus (stiffness) 73.1 GPa source typical not sourced Density 2,770 kg/m³ source nominal 960 kg/m³ source typical (specific gravity) Strength to weight 117 kN·m/kg 4.88x higher 24 kN·m/kg Stiffness to weight 26.4 MN·m/kg not sourced Poisson's ratio 0.33 source typical (handbook physical constant), all tempers 0.5 source government (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation 0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible). Shear modulus 27.5 GPa not sourced Bulk modulus 71.7 GPa not sourced Speed of sound 5,137 m/s not sourced Thermal Thermal conductivity 120 W/m·K source typical, 20 °C 0.151 W/m·K source government selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C Thermal expansion 22.9 µm/m·K source typical, mean 20-100 °C not sourced 100 mm part over a 50 °C swing 115 µm growth not sourced Specific heat 875 J/kg·K source typical, at 100 °C 1,881 J/kg·K source government (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C Heats up and cools (diffusivity) 49.5 mm²/s 592x faster 0.0836 mm²/s Thermal shock resistance 15,561 W/m not sourced Melting point 502–638 °C source melting range not sourced Max service temperature not sourced 70 °C source continuous use operating range Values for 2024-T4/T351, Kaiser Aluminum sheet, coil & plate typical datasheet; Poisson from MIL-HDBK-5J Weir Minerals Linatex Premium rubber (95 % natural rubber), typical physical properties, spec sheet WMD0118/202305
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions Is Aluminum 2024-T351 stronger than Rubber? Aluminum 2024-T351 is stronger: its yield strength is 324 MPa against tensile strength 23 MPa for Rubber (14.1x).
Which is lighter, Aluminum 2024-T351 or Rubber? Rubber is lighter: 960 kg/m³ against 2,770 kg/m³ for Aluminum 2024-T351.
Which is lighter for the same job, Aluminum 2024-T351 or Rubber? For the same stiffness or strength: Aluminum 2024-T351 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be Aluminum 2024-T351 Rubber Strong rod or tie lighter 4.88x heavier Strong beam lighter 2.02x heavier Strong panel or plate lighter 30% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which conducts heat better, Aluminum 2024-T351 or Rubber? Aluminum 2024-T351 conducts heat better: 120 W/m·K against 0.151 W/m·K for Rubber.
Among 59 materials 1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Aluminum Steel Iron Titanium Steel AISI 1018 Stainless 304 Stainless 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless 303 Stainless 17-4PH Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Aluminum 2024-T351 Stiffness against density 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Aluminum Steel Iron Titanium Steel AISI 1018 Stainless 304 Stainless 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless 303 Stainless 17-4PH Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick Aluminum 2024-T351 Rubber Strength against density