Materials / Compare

Aluminum 7075-T6 vs. Concrete

Compare Aluminum 7075-T6 vs. Concrete strength, stiffness, weight and thermal properties.

Change either side
Aluminum 7075-T6Wrought
ConcreteCast
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength503MPasourcetypical, 0.2% offset, .500 in dia specimennot sourced
Ultimate tensile strength572MPasourcetypicalnot sourced
Compressive strengthnot sourced27.6MPasourcespecified compressive strength class (f'c), not a measured typical
Elongation at break11%sourcetypical, in 4Dnot sourced
Young's modulus (stiffness)71GPasourcetypicalnot sourced
Density2,800kg/m³sourcenominal2,240–2,400kg/m³sourcerange for normalweight concrete
Strength to weight180kN·m/kgnot sourced
Stiffness to weight25.4MN·m/kgnot sourced
Poisson's ratio0.33sourcetypical (handbook physical constant)0.15–0.2sourcegeneral range at normal ambient conditions (overall 0.11-0.32)
Shear modulus26.7GPanot sourced
Bulk modulus69.6GPanot sourced
Speed of sound5,036m/snot sourced
Thermal
Thermal conductivity130W/m·Ksourcetypical, 20 °C, T6510.9W/m·Ksourcetypical (comparative value)
Thermal expansion23.4µm/m·Ksourcetypical, mean 20-100 °C8–12µm/m·Ksourcetypical range for portland cement concrete (aggregate dependent)
100 mm part over a 50 °C swing117µm growth50µm growth2.34x less
Specific heat960J/kg·Ksourcetypical, at 100 °C900J/kg·Ksourcetypical (NIST guidance for thermal analysis)
Heats up and cools (diffusivity)48.4mm²/s112x faster0.431mm²/s
Thermal shock resistance26,370W/mnot sourced
Melting point532–635°Csourcemelting rangenot sourced
Max service temperaturenot sourced65°Csourcecode long-term temperature limit (ASME Code, concrete containments)
Values for7075-T6/T651, Kaiser Aluminum rod & bar (mechanical) and sheet/coil/plate (physical) typical datasheets; Poisson from MIL-HDBK-5JNormal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC review

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Which is lighter, Aluminum 7075-T6 or Concrete?

Concrete is lighter: 2,320 kg/m³ against 2,800 kg/m³ for Aluminum 7075-T6.

Which conducts heat better, Aluminum 7075-T6 or Concrete?

Aluminum 7075-T6 conducts heat better: 130 W/m·K against 0.9 W/m·K for Concrete.

Which expands less with temperature?

Concrete expands less: 10 µm/m·K against 23.4 µm/m·K for Aluminum 7075-T6.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 7075-T6
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 7075-T6
Strength against density

Related comparisons